Effect of Ca element on oxygen content, wetting and spreading properties of Au–Ga filler metal
Source abstract
Abstract
Abstract To meet the low oxygen content requirement on filler metals used in high reliable vacuum brazing of power device, Ca was doped into the Au–Ga filler metal, and the effects of Ca on the oxygen content, the wetting and spreading properties of the filler metal were investigated. The results reveal that Ca can effectively decrease the oxygen content in the Au-Ga-Ca filler metal, and the wettability and spreadability of the Au-Ga-Ca filler metal on the Cu substrate were significantly improved. With 0.004 wt % of Ca addition, the oxygen content in the filler metal decreased to 0.0032 wt % and the spreading area increased to a peak value of74.6 mm2. Proper amount of Ca addition can also effectively restrain the growth of intermetallic compounds (IMC) layer at the vacuum brazed filler metal/Cu interface and improve the shear strength of the joints. For the Cu/Au-Ga-0.004Ca/Cu joints vacuum brazed at 480 °C and a vacuum degree of 5 × 10−3 mbar, the IMC/filler metal interface is flat and the IMC layer is uniform in thickness, and shear strength of the joint was 48.3 MPa, 49.5% higher than the Cu/Au–Ga/Cu joint. It is demonstrated that the Au-Ga-0.004Ca filler metal has the best combination property, and high ratio of brazed area can be obtained with Au-Ga-0.004Ca filler metal at a proper vacuum degree in brazing of real components.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Copper Interconnects and Reliability · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Evaluating IGBT temperature evolution during short circuit operations using a TSEP-based method
2. High power transistor frequency converter for supply of industrial transformer-type electron accelerators10.1016/S0042-207X(01)00219-6 ↗
3. Vianco · 2012
4. A comparative study on the microstructure and mechanical properties of Cu6Sn5 and Cu3Sn joints formed by TLP soldering with/without the assistance of ultrasonic waves10.1007/s11661-018-4664-6 ↗
5. Thermal materials solve power electronics challenges
6. Research progress of Au- and Ag- based mid-temperature brazing filler alloys for electronic industry
7. Microstructures and mechanical properties of Ti3Al/Ni-based superalloy joints brazed with AuNi filler metal10.1016/j.jmst.2019.04.015 ↗
8. Power electronic assemblies: thermo-mechanical degradations of gold-tin solder for attaching devices10.1016/j.microrel.2016.07.028 ↗
9. Effect of oxygen content on reliability of Au-20Sn solder joints for the chip-level package
10. Design and solderability characterization of novel Au-30Ga solder for high-temperature packaging10.1007/s10854-019-02787-8 ↗
11. Effects of surface microstructure on the active element content and wetting behavior of brazing filler metal during brazing Ti3SiC2 ceramic and Cu10.1016/j.vacuum.2018.07.043 ↗
12. Wetting and brazing characteristic of high nitrogen austenitic stainless steel and 316L austenitic stainless steel by Ag-Cu filler10.1016/j.vacuum.2019.04.064 ↗
13. Effect of joining temperature and bonding time on evolution of interfacial microstructure and brazing properties for 4J29/Ag-27Cu-4Ga/4J29 brazed joint10.1016/j.vacuum.2019.07.001 ↗
14. Oxidation resistant effects of Ag2S in Sn-Ag-Al solder: a mechanism for higher electrical conductivity and less whisker growth10.1016/j.corsci.2015.12.021 ↗
15. Role of cerium in microstructure and corrosion properties of Sn-1.0Ag solder alloys10.1016/j.matlet.2018.06.015 ↗
16. Effects of sulfur addition on the wettability and corrosion resistance of Sn-0.7Cu lead-free solder10.1016/j.microrel.2017.05.010 ↗
17. Effect of Ca on the microstructure and properties of Mg-6Al-1Nd alloy
18. Effect of Ca on corrosion resistance behavior of as-cast AZ91 magnesium alloys10.1016/S1875-5372(15)30009-6 ↗
19. Suppression of ignition and burning of molten Mg alloys by Ca bearing stable oxide film10.1023/A:1018526708423 ↗
20. Role of calcium alloying in magnesium alloys
21. Dynamic recrystallization and mechanical properties of high-strain-rate hot rolled Mg-5Zn alloys with addition of Ca and Sr10.1016/S1003-6326(19)65070-3 ↗
22. Effect of trace Ca on properties of AgCuZn solder
23. Effect of the microelements on the oxidation-resistance of Sn-0.7Cu lead-free solder
24. Wetting kinetic sand wettability enhancement of Pd added electrolytic Ni surface with molten Sn-3.0Ag-0.5Cu solder10.1016/j.matlet.2012.10.063 ↗
25. The role of oxide layers in solder joints10.1016/j.jallcom.2009.10.005 ↗