Effects of radio-frequency powers on the properties of carbon coatings on optical fibers prepared by thermal chemical vapor deposition enhanced with inductively coupled plasma
Source abstract
Abstract
Abstract This study investigates the effects of different radio-frequency (rf) powers on the characteristics of carbon coatings on optical fibers that are prepared by thermal chemical vapor deposition (thermal CVD) enhanced with inductively coupled plasma (ICP). Methane and nitrogen were used as the precursor gases, and rf-powers of ICP were set to 0, 50, 100, 200, 300, and 400 W. The deposition temperature, working pressure, and deposition time in the thermal CVD process were set to 1248 K, 4 kPa, and 2 h, respectively. Experimental results indicate that the deposition rate of carbon coatings increases as the rf-power increases from 0 to 200 W, but decreases as the rf-power exceeds 200 W. The mean crystallite size and ordered degree of carbon coatings decrease with increasing the deposition rate. Moreover, when the rf-power increases, the carbon coatings have more sp 2 carbon atoms and shift to graphite-like. With the assistance of ICP, carbon coatings can be deposited by thermal CVD at a low working pressure (about 4 kPa). Furthermore, the deposition rate and film properties can be adjusted by the rf-power.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics · Graphene research and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Diamond-like amorphous carbon10.1016/S0927-796X(02)00005-0 ↗
2. Mechanical strength and thermally induced stress voids of carbon-coated optical fibers prepared by plasma enhanced chemical vapor deposition method with different hydrogen/methane ratio10.1016/j.tsf.2004.12.059 ↗
3. Characterization of CVD carbon films for hermetic optical fiber coatings10.1016/S0257-8972(02)00888-5 ↗
4. Effects of deposition temperature on the properties of hermetically carbon-coated optical fibers prepared by thermal chemical vapor deposition10.1016/j.surfcoat.2007.05.043 ↗
5. Effects of hydrogen additive on microwave plasma CVD of nanocrystalline diamond in mixtures of argon and methane10.1016/j.diamond.2003.11.088 ↗
6. Paramagnetic properties and hydrogen-related structural relaxation effects in magnetron-sputtered a-C: H thin films10.1016/S0022-3093(01)01103-6 ↗
7. Evaluation of optical properties of the amorphous carbon film on fused silica10.1016/j.mseb.2003.10.013 ↗
8. Investigation of optical properties of a-C: H films deposited from acetylene using direct ion beam deposition method10.1016/j.vacuum.2005.01.092 ↗
9. Effects of radio-frequency powers on the properties of carbon coatings on optical fibers prepared by plasma enhanced chemical vapor deposition10.1016/j.surfcoat.2008.06.013 ↗
10. Improvement on the electrochemical characteristics of graphite anodes by coating of the pyrolytic carbon using tumbling chemical vapor deposition10.1016/S0013-4686(02)00845-9 ↗
11. Controlling the growth of CVD carbon from methane on transition metal substrates10.1016/j.surfcoat.2004.06.026 ↗
12. Effects of substrate size on properties of carbon coatings on glass cylinder substrates prepared by thermal chemical vapor deposition10.1016/j.tsf.2009.10.042 ↗
13. Effects of deposition parameters on characteristics of carbon coatings on optical fibers prepared by thermal chemical vapor deposition10.1016/j.surfcoat.2010.07.118 ↗
14. Effects of ammonia addition on thermal chemical vapor deposition rates and microstructures of carbon films10.1149/1.3591106 ↗
15. Kinetics of reactions in CH4/N2 afterglow plasma10.1016/S0042-207X(97)00066-3 ↗
16. Evaluation of the scavenging effect by low temperature laboratory plasmas driven with radio frequency10.1088/0741-3335/52/7/075014 ↗
17. CVD in hot wall reactors—the interaction between homogeneous gas-phase and heterogeneous surface reactions10.1002/(SICI)1521-3862(199807)04:04<151::AID-CVDE151>3.0.CO;2-2 ↗
18. Fabrication of amorphous carbon nitride films by hot-wire chemical vapor deposition10.1016/S0040-6090(01)01264-0 ↗
19. Chlorine-activated diamond chemical vapor deposition10.1149/1.2059312 ↗
20. Examination of the effects of nitrogen on the CVD diamond growth mechanism using in situ molecular beam mass spectrometry10.1016/S0925-9635(96)00647-4 ↗
21. Chemistry and kinetics of chemical vapour deposition of pyrocarbon: I. Fundamentals of kinetics and chemical reaction engineering10.1016/0008-6223(96)00010-3 ↗
22. Interpretation of Raman spectra of disordered and amorphous carbon10.1103/PhysRevB.61.14095 ↗
23. Effect of the substrate temperature on the deposition of hydrogenated amorphous carbon by PACVD at 35 kHz10.1016/S0040-6090(98)01002-5 ↗
24. General equation for the determination of the crystallite size La of nanographite by Raman spectroscopy10.1063/1.2196057 ↗
25. Surface modification of magnetic recording media by filtered cathodic vacuum arc10.1063/1.3245399 ↗
26. Direct evaluation of the sp3 content in diamond-like-carbon films by XPS10.1016/S0169-4332(98)00319-5 ↗