Abstract Large area electronics require large size thin films whose eventual inhomogeneities arise as a problem. Hydrogenated amorphous silicon carbide thin films (a-Si 1− x C x :H) for four different source gas mixtures at two power densities were deposited by plasma enhanced chemical vapor deposition (PECVD) technique. The degree of film homogeneity was investigated through measurements of deposition rate, refractive index and optical energy gap along the radial direction of bottom electrode. Both ellipsometer at various incident angles and optical transmittance at normal incidence were used in mutual control as diagnosing tools. It seems there is a critical power density beyond which inhomogeneities of the deposited films along the radial direction of the electrode are unavoidable.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Thin-Film Transistor Technologies · Phase-change materials and chalcogenides · Silicon Nanostructures and Photoluminescence
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Yu · Solar Energy Mater Solar Cells · 2001 · 66 · 15510.1016/S0927-0248(00)00168-9 ↗
2. Kruangam D, In: Kanicki J, editor. Amorphous and microcrystalline semiconductor devices, Boston: Artech House; 1991. p. 195.
3. Palma F, In: Street RA, Technology and Applications of Amorphous Silicon, Verlag: Springer, Berlin, 2000. p. 307.10.1007/978-3-662-04141-3 ↗
4. Solomon · Appl Surface Sci · 2001 · 184 · 310.1016/S0169-4332(01)00475-5 ↗
5. Schmitt · Plasma Sources Sci Technol · 2002 · 11 · A20610.1088/0963-0252/11/3A/331 ↗
6. Meiling · J Appl Phys · 1996 · 80 · 354610.1063/1.363227 ↗
7. Perrin · Plasma Phys Control Fusion · 2000 · 42 · B35310.1088/0741-3335/42/12B/326 ↗
8. Satake · Plasma Sources Sci Technol · 2004 · 13 · 43610.1088/0963-0252/13/3/010 ↗
9. Tikhonravov AV, Trubetskov MK, OptiChar Software 〈http://www.optilayer.com〉, Version 4.13, 2002.
10. Manifacier · J Phys E: Sci Instrum · 1976 · 9 · 100210.1088/0022-3735/9/11/032 ↗
11. Swanepoel · J Phys E: Sci Instrum · 1983 · 16 · 121410.1088/0022-3735/16/12/023 ↗
12. Akaoglu · Appl Opt · 2000 · 39 · 161110.1364/AO.39.001611 ↗
13. Tauc · Phys Status Solidi · 1966 · 15 · 62710.1002/pssb.19660150224 ↗
14. Armaou · Chemical Engineering Science · 1999 · 54 · 330510.1016/S0009-2509(98)00458-8 ↗
15. Robertson · Thin Solid Films · 1999 · 337 · 3210.1016/S0040-6090(98)01171-7 ↗
16. Robertson · J Appl Phys · 2000 · 87 · 260810.1063/1.372226 ↗
17. von Keudell · Plasma Sources Sci Technol · 2000 · 9 · 45510.1088/0963-0252/9/4/302 ↗
18. Kessels · Thin Solid Films · 2001 · 383 · 15410.1016/S0040-6090(00)01594-7 ↗
19. Dewarrat · Thin Solid Films · 2003 · 427 · 1110.1016/S0040-6090(02)01173-2 ↗
20. Hopf · J Appl Phys · 2000 · 87 · 271910.1063/1.372246 ↗
21. von Keudell · J Appl Phys · 1996 · 79 · 109210.1063/1.360796 ↗
22. Swhwartz-Selinger · J Appl Phys · 1996 · 86 · 398810.1063/1.371318 ↗
23. von Keudell · Appl Phys Lett · 2000 · 76 · 67610.1063/1.125858 ↗
24. von Keudell · Diamond Related Mater · 2002 · 11 · 96910.1016/S0925-9635(01)00553-2 ↗
25. Nguyen VS, in: Schuegraf KK, Handbook of Thin-Film Deposition Processes and Techniques, New York: Noyes Publications; 1988. p. 112.