Natural aging of Ni60Nb40 metallic glass thin film: Evolution of microstructure and mechanical properties
Source abstract
Abstract
Abstract Since metallic glass thin films (MGTFs) are commonly used in the atmosphere of air, the study on the evolution of structure, morphology, and mechanical properties of MGTFs exposed to air is of great significance for the practical application of MGTFs. The oxide formation mechanisms are investigated by experimental and calculation methods in this work. The results indicated that the crystalline oxide NiNb2O6 can be formed when exposed to air. The crystal structure of the oxide is orthorhombic, and the lattice constants can be calculated as: a = 14.022, b = 5.675 and c = 5.015 nm. The oxide NiNb2O6 was initiated around the amorphous island-like boundary during natural aging. The island boundary of amorphous matrix can provide the formation condition of nucleation and growth for crystalline oxide. The averaged Young's modulus and hardness of NiNb2O6 oxide are much higher than that of the amorphous matrix based on the results of experiments and first-principle calculations, indicating that the presence of crystalline oxides might improve the wear-resistance performance of the films.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · High-Temperature Coating Behaviors · Surface Roughness and Optical Measurements
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. High-modulus organic glasses prepared by physical vapor deposition10.1002/adma.200901673 ↗
2. Organic glasses with exceptional thermodynamic and kinetic stability10.1126/science.1135795 ↗
3. Influence of substrate temperature on the stability of glasses prepared by vapor deposition10.1063/1.2789438 ↗
4. Crystallization behavior upon heating and cooling in Cu50 Zr50 metallic glass thin films10.1016/j.actamat.2016.08.076 ↗
5. Effects of substrate temperature on structure, thermal stability and mechanical property of a Zr-based metallic glass thin film10.1016/j.tsf.2015.10.049 ↗
6. Ultrastable metallic glass10.1002/adma.201302700 ↗
7. Ultrastable metallic glasses formed on cold substrates10.1038/s41467-018-03656-4 ↗
8. Long-term stability of a horizontally-aligned carbon nanotube field emission cathode coated with a metallic glass thin film10.1016/j.carbon.2011.11.041 ↗
9. Influence of thin-film metallic glass coating on fatigue behavior of bulk metallic glass: experiments and finite element modeling10.1016/j.msea.2017.03.071 ↗
10. Wear resistivity of super-precision microgear made of Ni-based metallic glass10.1016/j.msea.2006.02.300 ↗
11. Design criteria for wear-resistant nanostructured and glassy-metal coatings10.1016/j.surfcoat.2003.09.011 ↗
12. Structural relaxation phenomenon in amorphous Al85Ni10Ce5 alloy during natural aging10.1023/A:1026330811839 ↗
13. Features of the formation of an oxide layer on the surface of amorphous Zr41.2Ti13.8Cu12.5Ni10.0Be22.5 alloy10.3103/S1062873810050047 ↗
14. Stress-state-dependent deformation behavior in Ni–Nb metallic glassy film10.1016/j.actamat.2012.04.028 ↗
15. Structure relaxation effect on hardness and shear transformation zone volume of a Ni Nb metallic glassy film10.1016/j.jnoncrysol.2018.07.050 ↗
16. Substrate temperature effect on growth behavior and microstructure-properties relationship in amorphous Ni Nb thin films10.1016/j.jnoncrysol.2018.12.023 ↗
17. Structure and properties of nanoglasses10.1002/adem.201800404 ↗
18. Thin-film growth dynamics with shadowing and re-emission effects10.1117/1.3543822 ↗
19. Influence of annealing on the structural and optical properties of gallium oxide films deposited on c-sapphire substrate10.1016/j.vacuum.2019.05.034 ↗
20. Na incorporated improved properties of Cu 2 ZnSnS 4 (CZTS) thin film by DC sputtering10.1016/j.vacuum.2018.05.007 ↗
21. Observation of field emission from carbon nanoparticles film coating on top of vertically aligned carbon nanotubes on silicon substrate10.1016/j.vacuum.2019.06.001 ↗
22. Lightweight refractory high entropy alloy coating by laser cladding on Ti–6Al–4V surface10.1016/j.vacuum.2020.109823 ↗
23. Loading rate effect on the creep behavior of metallic glassy films and its correlation with the shear transformation zone10.1016/j.msea.2014.11.022 ↗
24. First principles methods using CASTEP
25. VESTA3 for three-dimensional visualization of crystal, volumetric and morphology data10.1107/S0021889811038970 ↗
26. Tailoring nanostructured Ni-Nb metallic glassy thin films by substrate temperature10.1016/j.actamat.2020.04.046 ↗
27. Formation of nanostructured metallic glass thin films upon sputtering10.1016/j.heliyon.2016.e00228 ↗
28. Transition from a strong-yet-brittle to a stronger-and-ductile state by size reduction of metallic glasses10.1038/nmat2622 ↗
29. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
30. Microstructure and property of Fe–Co–B–Si–C–Nb amorphous composite coating fabricated by laser cladding process10.1016/j.apsusc.2013.04.077 ↗
31. Vitos · 2007