journal article·2020-11

The impact of oxygen content on the reliability of Au-20Sn solder hermetic package

Liujue Wang, Songbai Xue, Yaowei Lin, Hongneng Chen

Vacuum· Volume 181
Publisher page

Abstract

Abstract Hermetic sealing devices are produced with Au-20Sn solder at different oxygen content levels to study the reliability of the seal joints. Cross section of Au-20Sn solder joints processed with different oxygen content were examined by SEM, which shows that the microstructure displayed an obvious deterioration with the increase of oxygen content. It was found that bonding at 16 ppm oxygen content level, an uniform bonding interface with void-free was obtained with good hermeticity. However, when the oxygen content reached 55 ppm, voids and cracks were generated along the seal joint and the helium leak rate was higher than 5 × 10−8 atm cm3/s, which is the rejected limit value of MIL-STD-883 K. According to the reliability test results, we believe that the hermeticity deterioration is attributed to voids and cracks with the extension of aging time. In addition, samples with poor hermeticity were analyzed to know the failure mechanism of the seal joints and the feasible methods were proposed for improving hermeticity.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced materials and composites · Electrical Contact Performance and Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Fabrication and characterization of a low-temperature hermetic MEMS package bonded by a closed loop AuSn solder-line
2. Stability characterization of vacuum encapsulated MEMS resonators with Au–Sn solder bonding10.1007/s00542-018-3888-0 ↗
3. Wafer-level vacuum sealing by transfer bonding of silicon caps for small footprint and ultra-thin MEMS packages10.1109/JMEMS.2019.2910985 ↗
4. Localized silicon fusion and eutectic bonding for MEMS fabrication and packaging10.1109/84.825770 ↗
5. Wafer-level hermetic MEMS packaging by anodic bonding and its reliability issues10.1016/j.microrel.2014.02.001 ↗
6. Polymer integration for packaging of implantable sensors10.1016/j.snb.2014.05.063 ↗
7. A study on the optimization of anisotropic conductive films for Sn-3Ag-0.5Cu-based flex-on-board application at a 250 degrees C bonding temperature
8. A study on the bonding conditions and nonconductive filler contents on cationic epoxy-based Sn-58Bi solder ACFs joints for reliable flex-on-board applications
9. Effects of acrylic adhesives property and optimized bonding parameters on Sn58Bi solder joint morphology for flex-on-board assembly10.1016/j.microrel.2017.08.009 ↗
10. Research progress of micro-alloying Sn-Cu based lead-free solders
11. Research and application of silver-based brazing alloys in manufacturing industries: a review
12. Recent advances in nano-materials for packaging of electronic devices
13. Microstructural evolution of the Au–20 wt.% Sn solder on the Cu substrate during reflow
14. Microstructural evolution and orientation-correlated origin of the coarsening behaviors in Au–Sn eutectic alloys10.1016/j.jallcom.2019.07.337 ↗
15. Microstructure evolution and properties of rapidly solidified Au-20Sn eutectic solder prepared by single-roll technology10.1016/j.jallcom.2018.12.073 ↗
16. Microstructural evolution and shear performance of AuSn20 solder joint under gamma-ray irradiation and thermal cycling
17. Microstructure evolution and mechanical reliability of Cu/Au–Sn/Cu joints during transient liquid phase bonding10.1007/s10853-018-2204-9 ↗
18. Comparative study of Au–Sn and Sn–Ag–Cu as die‐attach materials for power electronics applications10.1002/sia.5998 ↗
19. Fluxless bonding of large silicon chips to ceramic packages using electroplated eutectic Au/Sn/Au structures10.1007/s11664-009-0861-9 ↗
20. Application of Au-Sn eutectic bonding in hermetic radio-frequency microelectromechanical system wafer level packaging10.1007/BF02690529 ↗
21. Investigation of interfacial reaction between Au-Sn solder and Kovar for hermetic sealing application10.1016/j.mee.2007.05.058 ↗
22. Fabrication and characterization of a low-temperature hermetic MEMS package bonded by a closed loop AuSn solder-line[C]//Micro Electro Mechanical Systems, 2003. MEMS-03 Kyoto
23. Hermetic packaging for implantable microsystems: effectiveness of sequentially electroplated AuSn alloy
24. Effect of Ca element on oxygen content, wetting and spreading properties of Au–Ga filler metal10.1016/j.vacuum.2020.109380 ↗
25. Effect of joining temperature and bonding time on evolution of interfacial microstructure and brazing properties for 4J29/Ag-27Cu-4Ga/4J29 brazed joint10.1016/j.vacuum.2019.07.001 ↗
26. Effects of surface microstructure on the active element content and wetting behavior of brazing filler metal during brazing Ti3SiC2 ceramic and Cu10.1016/j.vacuum.2018.07.043 ↗
27. Wetting and brazing characteristic of high nitrogen austenitic stainless steel and 316L austenitic stainless steel by Ag- Cu filler10.1016/j.vacuum.2019.04.064 ↗
28. 2016
29. Interface reaction and intermetallic compound growth behavior of Sn-Ag-Cu lead-free solder joints on different substrates in electronic packaging10.1007/s10853-018-2907-y ↗
30. Inhibition of intermetallic compounds growth at Sn–58Bi/Cu interface bearing CuZnAl memory particles (2–6 μm)10.1007/s10854-019-02784-x ↗
31. Au-In-based hermetic sealing for MEMS packaging for down-hole application10.1007/s11664-014-3131-4 ↗
32. Aging effect on defect evolution and shear strength of nano-silver solder joint