ECR plasma deposited a-SiCN:H as insulating layer in piezoceramic modules
Source abstract
Abstract
Abstract Highly resistive and sufficiently stiff insulation layers are an important prerequisite for the direct integration of piezoceramic modules into microstructured aluminium alloy sheets to produce smart adaptronic metal parts. In this study, we evaluate the mechanical and electrical properties of amorphous, hydrogenated silicon carbonitride films (a-SiCN:H) deposited by electron cyclotron resonance plasma CVD. First, we find the optimal process parameters for silicon substrates which we then transfer to electroded lead zirconate titanate (PZT) plates. Deposition rate, Young's modulus, stoichiometry and resistivity of a-SiCN:H films are determined by stylus profilometry, nanoindentation, X-ray photoelectron spectroscopy, elastic recoil detection analysis and current-voltage measurements, respectively. Under a 100 kHz bipolar pulsed substrate bias, 2 … 3 μm thick, well insulating films with Young's modulus ≈100 GPa are deposited at high rate of up to 7 μm/h. The electrical performance of a-SiCN:H films on PZT substrates is, to large extent, governed by the size and number of PZT roughness peaks, locally enhancing the field strength. Furthermore, we briefly address the deposition of the electrode layer on PZT. The selected material, sputter-deposited CuCr1Zr alloy, considerably improves the fracture strength of PZT substrates.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Diamond and Carbon-based Materials Research · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Smart metal sheets by direct functional integration of piezoceramic fibers in microformed structures10.1007/s00542-013-1836-6 ↗
2. Low temperature plasma enhanced chemical vapor deposition of thin films combining mechanical stiffness, electrical insulation, and homogeneity in microcavities10.1063/1.3474989 ↗
3. Mid-frequency PECVD of a-SiCN: H films and their structural, mechanical and electrical properties10.1016/j.vacuum.2012.04.001 ↗
4. Review - silicon nitride and silicon nitride-rich thin film technologies: trends in deposition techniques and related applications10.1149/2.0011710jss ↗
5. Tailored amorphous silicon carbide barrier dielectrics by nitrogen and oxygen doping10.1016/j.tsf.2012.11.141 ↗
6. Comprehensive comparison of electrical and reliability characteristics of various copper barrier films10.1116/1.3591340 ↗
7. Optimization of the molecular sieving properties of amorphous SiCXNY:H hydrogen selective membranes prepared by PECVD10.1140/epjst/e2015-02511-y ↗
8. Mechanical behavior related to various bonding states in amorphous Si–C–N hard films10.1016/j.surfcoat.2014.09.002 ↗
9. Determination of the critical strain in thin plasma CVD insulation layers using the barrel compression test
10. Electron resonance plasma sources and their use in plasma-assisted chemical vapor deposition of thin films
11. Plasma deposition of optical films and coatings: a review10.1116/1.1314395 ↗
12. Two kinds of defect centers observed in SiN films prepared by ECR plasma CVD method10.1016/0168-583X(89)90778-7 ↗
13. Optoelectronic and structural properties of amorphous silicon–carbon alloys deposited by low-power electron-cyclotron resonance plasma-enhanced chemical-vapor deposition10.1063/1.369679 ↗
14. Characteristics of low-temperature silicon nitride (SiNx:H) using electron cyclotron resonance plasma10.1016/S0038-1101(00)00086-1 ↗
15. Low temperature growth of silicon nitride by electron cyclotron resonance plasma enhanced chemical vapour deposition10.1016/S0040-6090(00)01628-X ↗
16. Influence of the multipolar magnetic field configuration on the density of distributed electron cyclotron resonance plasmas10.1088/0963-0252/6/1/008 ↗
17. Formation of silicon nitride gate dielectric films at 300°C employing radical chemical vapor deposition10.1116/1.1289549 ↗
18. Interpretation of stress variation in silicon nitride films deposited by electron cyclotron resonance plasma10.1116/1.1776179 ↗
19. High density plasma deposition of device quality silicon nitride. II. Effects of thickness on the electrical properties
20. Low temperature deposition of SiNx:H using SiH4–N2 or SiH4–NH3 distributed electron cyclotron resonance microwave plasma10.1116/1.589579 ↗
21. Deposition of SiNx:H thin films by the electron cyclotron resonance and its application to Al/SiNx:H/Si structures10.1063/1.366713 ↗
22. SiCN alloys deposited by electron cyclotron resonance plasma chemical vapor deposition10.1063/1.117887 ↗
23. Low hydrogen content silicon nitride films deposited at room temperature with an ECR plasma source10.1149/1.1787498 ↗
24. I-V characteristics of electron-cyclotron-resonance plasma-enhanced chemical-vapor-deposition silicon nitride thin films10.1063/1.356455 ↗
25. The influence of carbon on the structure and photoluminescence of amorphous silicon carbonitride thin films10.1016/j.tsf.2016.12.014 ↗
26. Defect structure of carbon rich a-SiC: H films and the influence of gas and heat treatments10.1063/1.368138 ↗
27. Silicon nitride thin films deposited by electron cyclotron resonance plasma enhanced chemical vapor deposition for micromechanical system applications10.1016/j.tsf.2008.03.010 ↗
28. Silicon nitride deposited by ECR–CVD at room temperature for LOCOS isolation technology10.1016/S0169-4332(03)00120-X ↗
29. Stress and strain in polycrystalline thin films10.1016/j.tsf.2007.03.007 ↗
30. Piezoelectric Ceramic Products · 2016
31. Low hydrogen content silicon nitride films from electron cyclotron resonance plasmas10.1063/1.355318 ↗
32. Analysis of a-SiCN: H films by X-ray photoelectron spectroscopy10.1016/j.vacuum.2016.09.016 ↗
33. Influence of surface processing on the fracture strength of structurally integrated PZT fibers in shaped sheet metal parts
34. Influence of electrode layers on the fracture strength of PZT ceramics10.4028/www.scientific.net/SSP.260.187 ↗
35. Study of the substrate bias in plasma depositions using an electron cyclotron resonance plasma10.1063/1.346217 ↗
36. Secondary electron emission from dielectric materials of a Hall thruster with segmented electrodes10.1063/1.1568344 ↗
37. Ion-induced secondary electron emission from MgO and Y2O3 thin films10.1016/j.vacuum.2009.06.021 ↗
38. Low temperature deposition of a-SiC: H thin films applying a dual plasma source process10.1016/j.tsf.2016.07.030 ↗
39. Prediction of dielectric reliability from I–V characteristics: Poole–Frenkel conduction mechanism leading to √E model for silicon nitride MIM capacitor10.1016/j.microrel.2003.12.007 ↗
40. Dielectric properties of amorphous hydrogenated silicon carbide thin films grown by plasma-enhanced chemical vapor deposition10.1063/1.1555676 ↗
41. Analysis of the oxygen contamination present in SiNx films deposited by electron cyclotron resonance10.1116/1.579835 ↗
42. Plasma-enhanced chemical vapor deposition of silicon dioxide deposited at low temperatures10.1149/1.2044242 ↗
43. Experimental analysis of the thermal annealing of hard a-C: H films10.1016/j.diamond.2014.03.005 ↗
44. Plasma-assisted atomic layer deposition: basics, opportunities, and challenges10.1116/1.3609974 ↗
45. Comparative experimental analysis of the a-C: H deposition processes using CH4 and C2H2 as precursors10.1063/1.2777643 ↗
46. Measurement and modeling of neutral, radical, and ion densities in H2-N2-Ar plasmas10.1063/1.4913623 ↗
47. Fundamental properties of a-SiNx:H thin films deposited by ICP-PECVD for MEMS applications10.1016/j.apsusc.2013.07.104 ↗
48. Correlation between composition and stress for high density plasma CVD silicon nitride films10.1149/1.3263906 ↗
49. A high-throughput PECVD reactor for deposition of passivating SiN layers
50. Effects of silver-based metal electroplate on fatigue properties of PZT ceramics10.1016/j.ijfatigue.2007.08.002 ↗
51. Fatigue failure characteristics of lead zirconate titanate piezoelectric ceramics10.1016/j.jeurceramsoc.2009.09.014 ↗
52. Experimental and numerical study on inherent sensory characteristics of piezoceramic micro parts during joining by forming in metal sheets