Effect of sintering temperature on the microstructure and properties of Ti/W–C reinforced Fe-based composites
Source abstract
Abstract
Abstract The effects of sintering temperature on the Ti/W–C phase evolution, microstructural change and wear properties of Fe-based composites were studied. The results show that Ti and W will generate unstable TixW1-x mesophase during the ball milling process, and the lattice constant of W increase from 3.1648 A to 3.5523 A. Furthermore, the in situ TiC and WC appear diffraction double peaks near the diffraction angle of 36° with the change of the sintering temperature. At the same time, as the sintering temperature approaches the Ti–Fe liquidus, the appearance of a large-sized reinforcing phase and the aggregation of Fe around it, synergistically improve the wear resistance of the material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Selective laser remelting of in-situ Al2O3 particles reinforced AlSi10Mg matrix composite: densification, microstructure and microhardness10.1016/j.vacuum.2021.110365 ↗
2. The measurement of the adhesion force between ceramic particles and metal matrix in ceramic reinforced-metal matrix composites10.1016/j.compositesa.2015.05.025 ↗
3. Effects of manganese on diffusion and wear behavior of ZTA particles reinforced iron matrix composites in vacuum10.1016/j.vacuum.2020.109408 ↗
4. Characterization of interfacial layer of ZTA ceramic particles reinforced iron matrix composites10.1016/j.jallcom.2018.01.199 ↗
5. Effect of WC content on microstructure and mechanical properties of Ni3Al-bonded cermets10.1016/j.ceramint.2015.12.058 ↗
6. Microstructure evolution, recrystallization and tribological behavior of TiC/WC composite ceramics coating10.1016/j.vacuum.2019.04.049 ↗
7. Phase evolution and wear resistance of in-situ synthesized (Cr, W)23C6-WC composite ceramics reinforced Fe-based composite coatings produced by laser cladding10.1016/j.vacuum.2021.110242 ↗
8. In-situ synthesis of TiC/Fe alloy composites with high strength and hardness by reactive sintering10.1016/j.jmst.2017.03.006 ↗
9. Local composite reinforcements of TiC/FeMn type obtained in situ in steel castings10.1016/j.acme.2019.05.004 ↗
10. In situ synthesis WC reinforced iron surface composite produced by spark plasma sintering and casting10.1016/j.matlet.2017.09.005 ↗
11. The effect of volume fraction of WC particles on wear behavior of in-situ WC/Fe composites by spark plasma sintering10.1016/j.ijrmhm.2017.08.009 ↗
12. Microstructure and mechanical properties of Al/(Ti,W)C composites prepared by microwave sintering10.1016/j.jallcom.2013.12.016 ↗
13. New production of (Ti, W)C-based cermets toughened by in-situ formed WC and twinned (Ti, W)C platelets: carbonization of the Nix(Ti0.6, W0.4)4C-type η phases10.1016/j.jallcom.2017.09.339 ↗
14. Microstructure of (W,Ti)C–Co system containing platelet WC10.1016/j.msea.2010.06.056 ↗
15. The FeTi (Iron-Titanium) system
16. The same chemical state of carbon gives rise to two peaks in X-ray photoelectron spectroscopy10.1038/s41598-021-90780-9 ↗
17. C 1s peak of adventitious carbon aligns to the vacuum level: dire consequences for material's bonding assignment by photoelectron spectroscopy10.1002/cphc.201700126 ↗
18. X-ray photoelectron spectroscopy: towards reliable binding energy referencing10.1016/j.pmatsci.2019.100591 ↗
19. Reliable determination of chemical state in x-ray photoelectron spectroscopy based on sample-work-function referencing to adventitious carbon: resolving the myth of apparent constant binding energy of the C 1s peak10.1016/j.apsusc.2018.04.226 ↗
20. Preparation of zinc ferrite by high-energy ball-milling and microstructure characterization by Rietveld's analysis10.1016/S0254-0584(03)00169-X ↗
21. ≤Microstructural Changes of (Ti,W)C Solid Solution Induced by Ball Milling.(pdf)>,.
22. Evidence of linear lattice expansion and covalency enhancement in rutile TiO2 nanocrystals10.1063/1.1790596 ↗
23. Thermodynamic and lattice parameter calculation of TiCx produced from Al-Ti-C powders by laser igniting self-propagating high-temperature synthesis10.1016/j.msea.2006.12.075 ↗
24. In situ fabrication of titanium carbide particulates-reinforced iron matrix composites10.1016/j.matdes.2011.03.031 ↗
25. Development of an abrasion resistant steel composite with in situ TiC particles10.1016/S0043-1648(01)00790-6 ↗
26. An in situ (W,Ti)C–Ni composite fabricated by SHS method10.1016/j.jnoncrysol.2008.01.002 ↗
27. Microstructural temperature gradient-driven diffusion: possible densification mechanism for flash sintering of zirconia?10.1016/j.ceramint.2018.09.311 ↗
28. Nanocrystalline/nanosized manganese substituted nickel ferrites – Ni1−xMnxFe2O4 obtained by ceramic-mechanical milling route10.1016/j.ceramint.2015.11.155 ↗
29. Self-propagating exothermic reactions: the synthesis of high-temperature materials by combustion10.1016/0920-2307(89)90001-7 ↗
30. Fe–W–C thermodynamics and in situ preparation of tungsten carbide-reinforced iron-based surface composites by solid-phase diffusion10.1016/j.ijrmhm.2016.02.001 ↗
31. Improving wear resistance and friction stability of FeNi matrix coating by in-situ multi-carbide WC-TiC via PTA metallurgical reaction10.1016/j.surfcoat.2019.124957 ↗
32. Characterization of microstructures in inconel 625 using X-ray diffraction peak broadening and lattice parameter measurements10.1016/j.scriptamat.2004.03.017 ↗
33. Strain induced phase formation, microstructural evolution and bandgap narrowing in strained TiO2 nanocrystals grown by ball milling10.1016/j.jallcom.2016.03.154 ↗
34. Stability of (Ti,M)C (M=Nb, V, Mo and W) carbide in steels using first-principles calculations10.1016/j.actamat.2011.09.051 ↗
35. Effect of Mo addition on microstructure and mechanical properties of (Ti,W)C solid solution based cermets10.1016/j.ijrmhm.2013.11.004 ↗
36. On the quantitative analysis of secondary carbide and carbon in (Ti1−xMx)C solid solutions via XRD measurements10.1016/j.ijrmhm.2007.10.001 ↗