Microstructure and properties of FeCrMo damping alloy brazing joint using Mn-based brazing filler

Haojiang Shi, Jiazhen Yan, Ning Li, Xin Zhu, Kangwei Chen, Lingfei Yu

Vacuum· Volume 159
Publisher page

Abstract

Abstract Vacuum brazing of FeCrMo damping alloy is carried out by using Mn Ni Cu Cr Co brazing filler at 1080 °C for different times (5, 15, 30, 60, and 120 min). The results reveal that the joint's interfacial microstructure brazed for 15 min consists of three zones: the FeCrMo substrate, Fe solid solution layer, and a brazing seam consisting of a (Mn, Ni) solid solution. Kirkendall vacancies are observed in the brazing seam when the joint is brazed for 120 min, due to the fact that Fe diffuses more quickly than Ni, Cu, and Mn. The specimen manifests the most optimal damping capacity when brazed for 60 min, and its lap-shear strength still reaches 426.7 MPa. The detailed mechanisms behind the formation of different phases across the brazed joint and their correlations with joint strength and damping capacity are also discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Shape Memory Alloy Transformations · Metal and Thin Film Mechanics · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Influence of alloy elements (Mo, Nb, Ti) on the strength and damping capacity of Fe-Cr based alloy10.1016/j.msea.2016.05.013 ↗
2. Effect of minor Zr element on microstructure and properties of Fe-16Cr-2.5Mo damping alloys10.1016/j.jallcom.2017.11.354 ↗
3. Effect of cooling rate on damping capacity of Fe–Cr based ferromagnetic metal alloy10.1016/j.msea.2015.10.086 ↗
4. Microstructural evolution and thermal stress relaxation of Al2O3/1Cr18Ni9Ti brazed joints with nickel foam10.1016/j.vacuum.2017.10.030 ↗
5. Interfacial microstructure and mechanical property of brazed copper/SiO2, ceramic joint10.1016/j.vacuum.2017.03.037 ↗
6. Zhang · 1998
7. Application of vacuum brazing as a metal joining technique10.1016/0042-207X(74)90062-1 ↗
8. Principles of soldering and brazing
9. Interdiffusion and microstructure evolution during brazing of austenitic martensitic stainless steel and aluminum-bronze with Ag-Cu-Zn based brazing filler material10.1016/j.jallcom.2018.01.043 ↗
10. Effect of domain variations on damping capacity of Fe-16Cr-2.5Mo alloy solution annealed at 1373 K and 1473 K10.1016/j.jmmm.2010.11.023 ↗
11. M.S. Blanter, I.S. Golovin, H. Neuhäuser, H.-R. Sinning. Internal Friction in Metallic Materials: a Handbook, Springer, pp. 4.
12. On relationship between annealing treatment and magnetostriction behavior of Fe–16Cr–2.5Mo damping alloy10.1016/j.jallcom.2013.08.070 ↗
13. Msit®, Materials Science International Team · 2007
14. International · 1992
15. 1992 · 938
16. Joining of 304SS and pure copper by rapidly solidified Cu-based braze alloy10.1016/j.fusengdes.2011.04.002 ↗
17. The microstructural evolution of infrared brazed Fe 3 Al by BNi-2 braze alloy10.1016/S0966-9795(02)00252-2 ↗
18. Effect of zinc addition on void formation in solid-liquid interdiffusion bonding of copper10.2320/matertrans.MD201509 ↗
19. Principles of soldering and brazing
20. Characterization of diffusion bonded joint between titanium and 304 stainless steel using a Ni interlayer10.1016/j.matchar.2007.05.015 ↗
21. Electrical and thermal properties of the interface at diffusion-bonded and soldered 304 stainless steel and copper bimetal10.1016/S0924-0136(03)00029-3 ↗
22. Microstructural evaluation of 410 SS/Cu diffusion-bonded joint10.1016/S1005-0302(10)60027-8 ↗
23. Diffusion bonding of 410 stainless steel to copper using a nickel interlayer10.1016/j.matchar.2010.03.006 ↗
24. Kinetics of high-temperature spreading10.1016/j.cossms.2006.04.005 ↗
25. Development of a copper-based filler alloy for brazing stainless steels10.1016/j.msea.2009.05.049 ↗
26. The microstructure and mechanical properties of 1Cr17Ni2/QAl7 brazed joints using Cu-Mn-Ni-Ag brazing alloy10.1016/j.msea.2016.03.020 ↗
27. Effect of quenching treatment on damping capacity of Fe-13Cr-2. 5Mo alloy