Deposition and characterization of MAX-phase containing Ti–Si–C thin films by sputtering using elemental targets
Source abstract
Abstract
Abstract Deposition of Ti–Si–C thin films onto glass substrates by magnetron DC-RF sputtering was examined using elemental targets of titanium, silicon and carbon, in order to investigate effects of carbon content in the films on the formation of ternary carbide compounds such as Ti 3 SiC 2 , known as MAX-phase. The DC and RF powers supplied for sputtering the titanium target and the silicon one were respectively fixed at DC120 W and RF50 W, while the DC power supplied for sputtering the carbon target was varied from 400 W to 200 W to vary the carbon content in the deposited films. Based on XRD, it was found that Ti 3 SiC 2 as well as TiC x were formed in the film obtained under an electric power of DC200 W while only TiC x formed under an electric power higher than DC300 W. According to Raman spectroscopy, it was found that excess carbon atoms precipitated out as fine graphite crystallites in the Ti–Si–C film, and it was assumed that its amount increased with increasing the carbon content in the film. The electrical resistivity of the obtained films decreased with the decrease of the electric power supplied to the carbon target, and the minimum electrical resistivity lower than 230 μΩcm was noteworthy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Choy · Mater Sci Eng · 2000 · A 278 · 481
2. Pecz · Appl Surf Sci · 2002 · 206 · 810.1016/S0169-4332(02)01195-9 ↗
3. Eklund · Phys Rev B · 2006 · 74 · 4541710.1103/PhysRevB.74.045417 ↗
4. Emmerlich · Acta Mater · 2007 · 55 · 147910.1016/j.actamat.2006.10.010 ↗
5. Barsoum · Am J Sci · 2001 · 89 · 33410.1511/2001.28.736 ↗
6. Barsoum · Interceram · 2000 · 49 · 226
7. Molina-Aldareguia · Scr Mater · 2003 · 49 · 15510.1016/S1359-6462(03)00214-8 ↗
8. Myhra · Mater Lett · 1999 · 39 · 610.1016/S0167-577X(98)00206-7 ↗
9. Barsoum · Prog Solid State Chem · 2000 · 28 · 20110.1016/S0079-6786(00)00006-6 ↗
10. Hoegberg · Surf Coat Technol · 2005 · 193 · 610.1016/j.surfcoat.2004.08.174 ↗
11. Voevodim · Diamond Relat Mater · 1998 · 7 · 46310.1016/S0925-9635(97)00214-8 ↗
12. Emmerlich · J Appl Phys · 2004 · 96 · 481710.1063/1.1790571 ↗
13. Sonoda · Jpn J. Appl Phys · 2012 · 5110.1143/JJAP.51.01AC06 ↗
14. Palmquist · Appl Phys Lett · 2002 · 81 · 33410.1063/1.1494865 ↗
15. Barsoum · Am Sci · 1996 · 79 · 1953
16. Eklund · J Vac Technol · 2005 · B 23 · 248610.1116/1.2131081 ↗
17. Palmquist · Phys Rev · 2004 · B 70 · 16540110.1103/PhysRevB.70.165401 ↗
18. Amer · J Appl Phys · 1998 · 84 · 581710.1063/1.368849 ↗
19. Rester · Mater Sci Eng · 2006 · A 429 · 9010.1016/j.msea.2006.05.053 ↗
20. Tuinstra · J Compos Mater · 1970 · 4 · 49210.1177/002199837000400405 ↗
21. Tuinstra · J Chem Phys · 1970 · 53 · 112610.1063/1.1674108 ↗
22. El-Raghy · J Am Ceram Soc · 1999 · 82 · 285510.1111/j.1151-2916.1999.tb02167.x ↗
23. Radovic · Acta Mater · 2000 · 48 · 45310.1016/S1359-6454(99)00351-1 ↗