Relation between microstructure and hardness of nano-composite CrN/Si3N4 coatings obtained using CrSi single target magnetron system
Source abstract
Abstract
Abstract Sintered targets with mixed Cr and Si (10, 20, 30, 35 and 40 at. %) elemental powders were sputtered in mixture of argon and nitrogen on silicon substrates kept either at ambient temperature or at 600 °C. The microstructure was characterized using transmission electron microscopy, while mechanical properties were estimated based on hardness measurements. Observations showed that magnetron sputtering of targets with high silicon content on substrates at ambient temperature resulted in the formation of gradient nano-composites that are partly amorphous and partly crystalline. The amorphous phase dominated in the zone close to the substrate, while the nano-crystalline character was more pronounced nearer to the coating surface. The volume of crystalline phase in the coatings was decreasing with increasing silicon content to such an extent that those obtained from CrSi40 target were fully amorphous. The coatings deposited on substrates resistively heated up to 600 °C showed fine columnar microstructure with diameter decreasing with increasing silicon content, which changed to nano-composite and eventually fully amorphous for those obtained using CrSi35 and CrSi40 targets. The Elemental mapping by electron energy filtered imaging helped prove that in the nano-composite coatings the CrN–type crystalline phase and the amorphous phase are enriched respectively in chromium and silicon. The hardness of the coatings deposited at ambient temperature and characterized by mixed crystalline and amorphous microstructure was close to 20 GPa, except those containing layers enriched in chromium and silicon, which fall down to 15 GPa or even 10 GPa. The hardness of crystalline coatings deposited at 600 °C was increasing from 20 to 30–35 GPa with decreasing average column diameter from ∼40 to ∼35 and ∼25 nm (obtained from CrSi10, CrSi20 and CrSi30 targets). The higher silicon content in the coatings caused both further diminishing of the average crystallite size below 10 nm and simultaneous formation of an amorphous phase. The hardness of the coatings with such nano-composite microstructure was however decreased to ∼25 GPa. Finally, the hardness of fully amorphous coatings obtained from CrSi40 target under the same deposition conditions was at the level of 10 GPa. Our experiments proved that it is possible to obtain extremely fine columnar (Cr,Si)N coatings twice as hard as pure CrN, although a basic one target magnetron system and oxygen-contaminated CrSi targets were only used.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Ti–Si–N films prepared by plasma enhanced chemical vapor deposition10.1007/BF01447027 ↗
2. A concept for the design of novel superhard coatings10.1016/0040-6090(95)06695-0 ↗
3. New development in superhard coatings: the superhard nanocrystalline–amorphous composites10.1016/S0040-6090(97)00665-2 ↗
4. Structural properties, internal stress and thermal stability of nc- TiN/a – Si3N4, nc–TiN/TiSix and nc–(Ti1-yAlySix) N superhard nanocomposite coatings reaching the hardness of diamond10.1016/S0257-8972(99)00451-X ↗
5. Structure and mechanical properties of Ti–Si–N ceramic nanocomposite coatings10.1016/S0257-8972(02)00603-5 ↗
6. Comparative investigation of Ti–Si–N films magnetron sputtered using Ti5Si3+Ti and Ti5Si3+TiN targets10.1016/j.surfcoat.2003.08.052 ↗
7. Deposition and mechanical properties of Ti–Si–N coated layer on WC–Co by RF inductively coupled plasma–enhanced chemical vapor deposition10.1016/S0040-6090(02)00841-6 ↗
8. Improving the properties of titanium nitride by incorporation of silicon10.1016/S0257-8972(98)00560-X ↗
9. A quantitative study of the hardness of a superhard nanocrystalline titanium nitride/silicon nitride coating10.1016/j.scriptamat.2005.02.024 ↗
10. The issue of the reproducibility of deposition of superhard nanocomposites with hardness of ≥ 50 GPa10.1016/j.surfcoat.2004.11.023 ↗
11. Composition, nanostructure and origin of the ultrahardness in nc-TiN/a-Si3N4 and nc-TiSi2 nanocomposites with HV 80 to 105 GPa10.1016/S0257-8972(00)00957-9 ↗
12. Nanocomposite hard coatings for wear protection10.1557/mrs2003.59 ↗
13. Mechanical and tribological properties of Cr–N and Cr–Si–N coatings reactively sputter deposited10.1016/j.surfcoat.2005.02.214 ↗
14. Effect of silicon additions in CrSi (10, 20, 30, 40 at. %) magnetron targets on microstructure of reactively deposited (Cr, Si)N coatings10.4028/www.scientific.net/SSP.186.182 ↗
15. Electrical, optical and mechanical properties of sputtered CrNy and Cr1-xSiXN1.02 thin films10.1016/S0040-6090(03)01113-1 ↗
16. Microstructure and mechanical properties of Cr–Si–N coatings prepared by pulsed reactive dual magnetron sputtering10.1016/j.surfcoat.2008.02.014 ↗
17. Synthesis and mechanical properties of Cr-Si-N coatings deposited by hybrid system of arc ion plating and sputtering techniques10.1016/j.surfcoat.2004.08.045 ↗
18. Different approaches to superhard coatings and nanocomposites10.1016/j.tsf.2004.10.053 ↗
19. Microstructure of novel superhard nanocrystalline – amorphous composites as analyzed by high resolution transmission electron microscopy10.1116/1.589778 ↗
20. Phase stabilities of self-organized nc-TiN/a-Si3N4 nanocomposites and Ti1-xSixNy solid solutions studied by ab-initio calculation and thermodynamic modelling10.1016/j.tsf.2007.07.134 ↗
21. Influence of substrate temperature and deposition rate on structure of thick sputtered Cu coatings10.1116/1.568682 ↗
22. Titanium nitride with silikon additions for tribological applications10.1002/sia.3463 ↗
23. Consolidating conditions of Cr-Si compacts and their microstructure