Phase stability of SiC against Ti at high temperature

Masaaki Naka, Jicai Feng, Julius C. Schuster

Vacuum· Volume 83· Issue 1
Publisher page

Abstract

SiC to SiC were reacted by Ti foil at high temperature of 1673 K in vacuum. Ti reacted with SiC, and formed many reaction phases between SiC and Ti. At 1673 K SiC reacted at a reaction time of 0.5 ks or longer. From the SiC many reaction zones of Ti3SiC2, Ti5Si3CX, Ti5Si3CX + TiC, and TiC + Ti were formed. Ti binary compound of TiC and Ti ternary compounds of Ti3SiC2, and Ti5Si3CX, were formed. The principle of the reaction zones was thermodynamically discussed by the corresponding chemical potential diagram.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (4)

Show source-provided references
1. Smith · 1990 · 35
2. Martineau · J Mater Sci · 1984 · 19 · 274910.1007/BF00550832 ↗
3. Morozumi · J Mater Sci · 1985 · 20 · 397610.1007/BF00552387 ↗
4. Yokokawa · Materia, Japan Inst Metals · 1996 · 35