Improved wear resistance of WS2 film by LT-deposited Ti interlayer with ω phase structure
Source abstract
Abstract
Abstract The goal of this paper was to investigate the structural/mechanical properties of arc-ion-plated Ti film deposited at ultralow temperature (166 K, LT-Ti film) and its effect as an interlayer on the wear resistance of sputtered WS2 film. The results revealed that the LT-Ti film mainly exhibited ω-phase structure due to the insufficient mobility of Ti adatoms at LT surface, while the α-phase was predominated in the Ti film deposited at room temperature (RT-Ti film). The LT-Ti film showed a higher hardness than the RT-Ti film as well as the better toughness and film-substrate adhesion on steel substrates. The wear resistance of sputtered WS2 film could be significantly improved by employing the Ti films as its interlayer, especially for the LT-Ti film.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Electrical Contact Performance and Analysis · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. The α→ω and β→ω phase transformations in Ti–Fe alloys under high-pressure torsion10.1016/j.actamat.2017.10.051 ↗
2. An overview on the use of titanium in the aerospace industry10.1016/0921-5093(96)10233-1 ↗
3. Interface microstructure of titanium thin-film/silicon single-crystal substrate correlated with electrical barrier heights10.1063/1.349641 ↗
4. Textor · 2001 · 172
5. Growth feature of ionic nitrogen doped CNx bilayer films with Ti and TiN interlayer by pulse cathode arc discharge10.1016/j.apsusc.2015.11.106 ↗
6. Frictional behavior of self-adaptive nanostructural Mo-Se-C coatings in different sliding conditions10.1016/j.wear.2013.03.032 ↗
7. Ultra-low friction W-S-N solid lubricant coating10.1016/j.surfcoat.2013.06.026 ↗
8. Dependence of stress-induced omega transition and mechanical twinning on phase stability in metastable β Ti–V alloys10.1016/j.matchar.2015.06.038 ↗
9. Morphological study of magnetron sputtered Ti thin films on silicon substrate10.1016/j.matchemphys.2008.04.048 ↗
10. Structure of nanometer-size crystalline Ti film10.1016/0965-9773(94)90116-3 ↗
11. Growth and structure of Ti films deposited on chemically polished MgO (100) substrates10.1016/S0022-0248(96)00685-9 ↗
12. Tayloy · 1961
13. Synthesis and characterization of nanocrystalline ZrNxOy thin films on Si by ion plating10.1016/j.surfcoat.2006.12.007 ↗
14. Improvement of anti-oxidation capability and tribological property of arc ion plated Ag film by alloying with Cu10.1016/j.apsusc.2011.03.154 ↗
15. A structure zone diagram including plasma-based deposition and ion etching10.1016/j.tsf.2009.10.145 ↗
16. Epitaxial growth of titanium thin films10.1116/1.1315691 ↗
17. Influence of condensation temperature on microstructure and tensile properties of titanium sheet produced by high-rate physical vapor deposition process10.1007/BF02649600 ↗
18. Structure, morphology and chemical composition of sputter deposited nanostructured Cr-WS2 solid lubricant coatings10.1016/j.surfcoat.2010.07.050 ↗
19. Structural, mechanical and tribological investigations of sputter deposited CrN-WS2 nanocomposite solid lubricant coatings10.1016/j.triboint.2011.07.007 ↗
20. Response of RF-sputtered MoS2 composite films to LEO space environment10.1016/j.vacuum.2017.07.021 ↗
21. Changes in the composition, structure and friction property of sputtered MoS2 films by LEO environment exposure10.1016/j.apsusc.2014.12.175 ↗
22. Growth, Structure and friction behavior of titanium doped tungsten disulphide (Ti-WS2) nanocomposite thin films10.1016/j.tsf.2009.02.103 ↗