Study of Nd-doping effect and mechanical cracking on photoreactivity of TiO2 thin films

J.O. Carneiro, V. Teixeira, A. João, A. Magalhães, C.J. Tavares

Vacuum· Volume 82· Issue 12
Publisher page

Abstract

Abstract Pure and Nd-doped TiO 2 thin films were fabricated by reactive d.c. magnetron sputtering at low-temperature from a pure Ti target. The structure of films was analyzed by X-ray diffraction (XRD). In order to study the Nd-doping effect on TiO 2 photocatalytic activity, some films were deposited on microscope glass substrates under a constant total sputtering pressure and using different Nd-doping concentrations. The effect of different Nd-dopant concentrations and its influence on the photocatalytic efficiency has been explored by measuring the photodegradation of rhodamine-B (RhB) aqueous solution under radiation of UV light. It is principally that for comparison between heat treatment and doping process on TiO 2 photocatalytic efficiency (important under the point of view of energy costs related with industrial sputtering techniques), crystalline TiO 2 films were also produced by thermal annealing. It was found that comparing with annealed pure TiO 2 films, Nd-doping do not improve the photocatalytic activity. At the same time, it was observed that there seems to exist a dopant concentration band for optimal photoreactivity. In order to study the effect of the film mechanical strength on photocatalytic activity, fragmentation tensile tests were also done on TiO 2 /PET (polyethylene terephthalate) substrates at increasing applied strains. It was found that increasing the magnitude of the applied tensile strain, pure TiO 2 becomes more photocatalytic efficient.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: TiO2 Photocatalysis and Solar Cells · Advanced Photocatalysis Techniques · Copper-based nanomaterials and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Ollis · 1993
2. Suri · Environ Eng · 1999 · 125 · 89710.1061/(ASCE)0733-9372(1999)125:10(897) ↗
3. Peill · Environ Sci Technol · 1996 · 30 · 280910.1021/es960047d ↗
4. Hoffmann · Chem Rev · 1995 · 95 · 6910.1021/cr00033a004 ↗
5. Bard · J Phys Chem · 1979 · 83 · 314610.1021/j100487a017 ↗
6. Fox · Acc Chem Res · 1983 · 16 · 31410.1021/ar00093a001 ↗
7. Nosaka · J Phys Chem · 1988 · 92 · 189310.1021/j100318a039 ↗
8. Wang · Nature · 1997 · 388 · 43110.1038/41233 ↗
10. Wang · J Phys Chem B · 1999 · 103 · 218810.1021/jp983386x ↗
11. Shah · 2001
12. Carneiro · Vacuum · 2005 · 78 · 3710.1016/j.vacuum.2004.12.012 ↗
13. Suzuki · Appl Phys Lett · 2001 · 78 · 396810.1063/1.1380730 ↗
14. Ohring · 1992
15. Thornton · Thin Solid Films · 1989 · 171 · 510.1016/0040-6090(89)90030-8 ↗
16. Yanaka · J Mater Sci · 1998 · 33 · 211110.1023/A:1004371203514 ↗
17. Reynaud · Surf Interface Anal · 2000 · 30 · 18510.1002/1096-9918(200008)30:1<185::AID-SIA862>3.0.CO;2-D ↗
18. Hsueh · J Am Ceram Soc · 1985 · 68 · 24110.1111/j.1151-2916.1985.tb15316.x ↗