Effects of O addition on the thermal behaviour of hard W–N sputtered coatings
Source abstract
Abstract
Abstract The structural thermal behaviour of three W–O–N sputtered coatings with similar metalloid to metal ratio (∼2.1) was investigated up to 900 °C after annealing in a vacuum tube furnace as well as in-situ HT-XRD under a controlled atmosphere of Ar–5%H2. The as-deposited microstructure of the coatings consisting in a nanocomposite of low-order W–O and W–N phases evaluated differently as a function of the oxygen content. The W–O–N film containing more than 27 at.% O delaminated severely from the steel substrates for temperatures as low as 500 °C. In opposite, for the coatings with less O content, the low range order of the as-deposited structure was maintained up to 800 °C and with further annealing crystallized into a mixture of WO2 and W2N. The thermal behaviour of the oxynitride films overcame that observed for oxygen-free nitride ones. This is due to the greater N content retaining during annealing treatment, in opposite to the W–N films which give rise to the single metallic α-W phase. The structural and compositional evolution supported the hardness behaviour obtained by the thermal treatment in protective ambiance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Copper Interconnects and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Polcar · Wear · 2007 · 262 · 65510.1016/j.wear.2006.07.010 ↗
2. Polcar · Wear · 2008 · 265 · 31910.1016/j.wear.2007.10.011 ↗
3. Louro · J Electrochem Soc · 1997 · 144 · 25910.1149/1.1837394 ↗
4. Cavaleiro · Surf Coat Technol · 2000 · 131 · 44110.1016/S0257-8972(00)00784-2 ↗
5. Parreira · Surf Coat Technol · 2006 · 200 · 651110.1016/j.surfcoat.2005.11.020 ↗
6. Antunes · Surf Coat Technol · 2002 · 149 · 2710.1016/S0257-8972(01)01413-X ↗
7. Louro · Surf Coat Technol · 1999 · 116-119 · 12110.1016/S0257-8972(99)00202-9 ↗
8. Vaz · Thin Solid Films · 2004 · 469-470 · 1110.1016/j.tsf.2004.06.191 ↗
9. Fenker · Surf Coat Technol · 2005 · 200 · 135610.1016/j.surfcoat.2005.08.074 ↗
10. Banakha · J Vac Sci Technol · 2006 · A 24 · 1
11. Wagner · J Vac Sci Technol · 1974 · 11 · 58210.1116/1.1318073 ↗
12. Reid · Thin Solid Films · 1993 · 236 · 31910.1016/0040-6090(93)90689-M ↗
13. Shen · Thin Solid Films · 2000 · 372 · 25710.1016/S0040-6090(00)01041-5 ↗
14. Ferreira · Key Eng. Mater. · 2002 · 230/232 · 64010.4028/www.scientific.net/KEM.230-232.640 ↗
15. Shen · Mat Sci Eng · 2000 · B76 · 10710.1016/S0921-5107(00)00424-4 ↗