Thermomechanical properties and oxidation resistance of Ce–Si alloyed Ti–Al–N thin films
Source abstract
Abstract
Abstract Within this study, we show that single-phase face centered cubic (fcc) Ti0.47Al0.46Ce0.02Si0.05N coatings (sputtered from Ti0.37Al0.57Ce0.02Si0.04 targets plus the addition of Ti) outperform their single-phase fcc Ti0.49Al0.51N counterparts (sputtered from Ti0.40Al0.60 targets plus the same addition of Ti). The deposition rate increases by more than 43% and also the hardness of as-deposited Ti0.47Al0.46Ce0.02Si0.05N coatings is with 39.9 ± 1.2 GPa (on sapphire) 13% higher. Furthermore, this Ce–Si alloyed coating shows a remarkably higher thermal stability, represented by a higher annealing temperature (1200 °C instead of 900 °C) after which hexagonal structured wurtzite-type AlN (w-AlN) can be detected. They also show a more parabolic like oxide growth rate (4.13·10−7 and 1.13·10−5 μm2/s at 850 and 950 °C) during the 10-h-oxidation experiment, whereas that of Ti0.49Al0.51N is close to linear already at 850 °C (especially after ∼2 h). The postponed w-AlN formation guarantees that the hardness of Ti0.47Al0.46Ce0.02Si0.05N is still 40.8 ± 1.6 GPa even after annealing at 1100 °C. Our results clearly demonstrate that the addition of 2 mol% CeSi2 to Ti–Al targets allows to increase the sputter rate and leads to Ce–Si alloyed nitride coatings with improved thermomechanical properties and oxidation resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Semiconductor materials and devices · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. On structure and properties of sputtered Ti and Al based hard compound films10.1116/1.573708 ↗
2. Titanium aluminum nitride films: a new alternative to TiN coatings10.1116/1.573713 ↗
3. Effects of aluminum concentration on the oxidation behaviors of reactively sputtered TiAlN films10.1111/j.1151-2916.1999.tb01819.x ↗
4. Characterization of thermally treated TiAlSiN coatings by TEM and nanoindentation10.1016/j.surfcoat.2004.08.060 ↗
5. Formation and diffusion properties of oxide films on metals and on nitride coatings studied with Auger electron spectroscopy and X-ray photoelectron spectroscopy10.1016/0040-6090(90)90216-Z ↗
6. Avoiding the high-temperature decomposition and softening of (Al1−xTix)N coatings by the formation of stable superhard nc-(Al1−xTix)N/a-Si3N4 nanocomposite10.1016/j.msea.2003.08.052 ↗
7. Industrial applications of superhard nanocomposite coatings10.1016/j.surfcoat.2008.05.038 ↗
8. Physical, structural and mechanical characterization of Ti1−xSixNy films10.1016/S0257-8972(98)00620-3 ↗
9. Some consequences of the partial crystallographic coherence between nanocrystalline domains in Ti–Al–N and Ti–Al–Si–N coatings10.1016/j.tsf.2006.02.092 ↗
10. Increased thermal stability of Ti-Al-N thin films by Ta alloying10.1016/j.surfcoat.2011.07.009 ↗
11. Influence of Nb on the phase stability of Ti–Al–N10.1016/j.scriptamat.2010.06.020 ↗
12. Effect of Hf on structure and age hardening of Ti–Al-N thin films10.1016/j.surfcoat.2011.11.020 ↗
13. Influence of Zr on structure, mechanical and thermal properties of Ti–Al–N10.1016/j.tsf.2011.03.139 ↗
14. Improvement on thermal stability of TiAlSiN coatings deposited by IBAD10.1080/02670844.2017.1341110 ↗
15. Influence of Si content on mechanical and tribological properties of TiAlSiN PVD coatings at elevated temperatures10.1016/j.surfcoat.2017.05.014 ↗
16. Microstructure and mechanical properties of nanocomposite (Ti,Si,Al)N coatings10.1016/S0040-6090(01)01348-7 ↗
17. Correlation between microstructure evolution and high temperature properties of TiAlSiN hard coatings with different Si and Al content10.1016/j.apsusc.2014.06.057 ↗
18. Different approaches to superhard coatings and nanocomposites10.1016/j.tsf.2004.10.053 ↗
19. Effect of sputtering target power on microstructure and mechanical properties of nanocomposite nc-TiN y a-SiN x thin films10.1016/S0040-6090(03)01125-8 ↗
20. Architecture of PVD coatings for metalcutting applications: a review10.1016/j.surfcoat.2014.08.068 ↗
21. Fracture toughness of Ti-Si-N thin films10.1016/j.ijrmhm.2017.12.015 ↗
22. Cerium doping of Ti–Al–N coatings for excellent thermal stability and oxidation resistance10.1016/j.surfcoat.2017.07.037 ↗
23. Atom assisted sputtering yield amplification10.1116/1.578049 ↗
24. Phase stability, mechanical properties and thermal stability of Y alloyed Ti–Al–N coatings10.1016/j.surfcoat.2013.07.030 ↗
25. Fischer-Cripps · 2011
26. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
27. Composition driven phase evolution and mechanical properties of Mo–Cr–N hard coatings10.1063/1.4926734 ↗
28. Critical review of analysis and interpretation of nanoindentation test data10.1016/j.surfcoat.2005.03.018 ↗
29. Ab initio-guided development of super-hard Mo–Al–Cr–N coatings10.1016/j.scriptamat.2017.06.052 ↗
30. TiAlN coatings deposited by triode magnetron sputtering varying the bias voltage10.1016/j.apsusc.2011.02.027 ↗
31. Compositional and structural evolution of sputtered Ti-Al-N10.1016/j.tsf.2009.04.056 ↗
32. Influence of oxygen impurities on growth morphology, structure and mechanical properties of Ti–Al–N thin films10.1016/j.tsf.2016.01.039 ↗
33. Structure and properties of Al–Ti–Si–N coatings prepared by the cathodic arc ion plating method for high speed cutting applications10.1016/S0257-8972(01)01391-3 ↗
34. Galileo comes to the surface!
35. Self-organized nanostructures in the Ti–Al–N system10.1063/1.1608464 ↗
36. Energetic balance and kinetics for the decomposition of supersaturated Ti1−xAlxN10.1016/j.actamat.2006.09.045 ↗
37. Decomposition pathways in age hardening of Ti–Al–N films10.1063/1.3610451 ↗
38. Growth of hard amorphous TiAlSiN thin films by cathodic arc evaporation10.1016/j.surfcoat.2013.07.014 ↗
39. Structure and thermal stability of arc evaporated (Ti0.33Al0.67)1 - xSixN thin films10.1016/j.tsf.2008.08.126 ↗
40. Improved thermal stability and oxidation resistance of Al-Ti-N coating by Si addition10.1016/j.tsf.2014.01.072 ↗