Geometrical outline evolution and size-inhibiting interaction of interfacial solder bubbles and IMCs during multiple reflows
Source abstract
Abstract
Abstract By utilizing synchrotron radiation X-ray imaging technique for in situ observation, the geometrical outline evolution and size-inhibiting interaction of solder bubbles and IMCs during multiple reflows were investigated in this work. It was found that the interfacial bubbles can inhibit the growth of IMC grains caused by the hindering effect of bubbles on contact and reaction between solder and substrate; meanwhile, following the growth of IMC grains, the bubble size in return got smaller and its aspect ratio became larger with reflow cycle, which is the result of inhibiting effect of solid IMC grains on solder voids; Because of boundary segregation and thermomigration, Cu atoms tend to gather on the bubble boundary and form a Cu-rich phase, consequently resulting in the formation of IMCs at the gas/solder interface area.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Metallurgical Processes and Thermodynamics · Solidification and crystal growth phenomena
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Reliability challenges in 3D IC packaging technology10.1016/j.microrel.2010.09.031 ↗
2. Through-silicon via and die stacking technologies for microsystems-integration
3. Fabrication and evaluation of 3D packages with through hole via
4. Thermo-mechanical simulations for 4-layer stacked IC packages
5. Microcontacts with sub-30μm pitch for 3D chip-on-chip integration10.1016/j.mee.2006.09.026 ↗
6. Numerical analysis of thermo-mechanical reliability of through silicon vias (TSVs) and solder interconnects in 3-dimensional integrated circuits10.1016/j.mee.2009.07.022 ↗
7. Transition from flip chip solder joint to 3D IC microbump: its effect on microstructure anisotropy10.1016/j.microrel.2012.07.029 ↗
8. Through-wafer electroplated copper interconnect with ultrafine grains and high density of nanotwins
9. Study of 15μm pitch solder microbumps for 3D IC integration
10. Bonding and electromigration of 30μm fine pitch micro-bump interconnection
11. Nonlinear thermal stress/strain analyses of copper filled TSV (through silicon via) and their flip-chip microbumps10.1109/TADVP.2009.2021661 ↗
12. Effect of wet pretreatment on interfacial adhesion energy of Cu-Cu thermocompression bond for 3D IC packages10.1007/s11664-009-0942-9 ↗
13. Voiding in BGAs10.1108/eb037911 ↗
14. Void formation mechanism of flip chip in package using no-flow underfill10.1115/1.3153369 ↗
15. A numerical study of void nucleation and growth in a flip chip assembly process10.1088/0965-0393/18/6/065005 ↗
16. The effect of a micro bubble dispersed gas phase on hydrogen isotope transport in liquid metals under nuclear irradiation10.1016/j.fusengdes.2013.08.004 ↗
17. Effect of electromigration on interfacial reactions between electroless Ni-P and Sn?3.5% Ag solder10.1016/j.tsf.2004.05.042 ↗
18. Effect of three-dimensional current and temperature distributions on void formation and propagation in flip-chip solder joints during electromigration10.1063/1.2220550 ↗
19. In situ observation of the void formation-and-propagation mechanism in solder joints under current-stressing10.1016/j.actamat.2005.01.014 ↗
20. Electromigration-induced UBM consumption and the resulting failure mechanisms in flip-chip solder joints10.1007/BF02692561 ↗
21. Effect of current crowding on whisker growth at the anode in flip chip solder joints10.1063/1.2822446 ↗
22. Effects of preexisting voids on electromigration failure of flip chip solder bumps10.1016/S0026-2692(01)00033-7 ↗
23. In-situ study on the formation and evolution behavior of voids at the interface during soldering process by synchrotron radiation real-time imaging technology
24. In situ study on growth behavior of interfacial bubbles and its effect on interfacial reaction during a soldering process10.1016/j.apsusc.2014.03.003 ↗
25. In situ study on growth behavior of interfacial bubbles and its size effect on Sn-0.7 cu/Cu interfacial reaction
26. Modeling the diffusion-driven growth of a pre-existing gas bubble in molten tin10.1007/s12540-015-4528-1 ↗
27. A numerical study of void nucleation and growth in a flip chip assembly process10.1088/0965-0393/18/6/065005 ↗
28. Thermomigration in Pb-free SnAg solder joint under alternating current stressing10.1063/1.3089872 ↗
29. Shewmon · 2016
30. The gorsky effect, electrotransport and thermotransport of hydrogen in metals10.1016/0022-5088(76)90042-4 ↗
31. Linear rate of grain growth in thin films during deposition10.1103/PhysRevB.67.245408 ↗
32. Bubble formation modeling in IE-911
33. Nucleation of gas bubbles in surface irregularities10.1080/00986449808912376 ↗