Abstract Cr–2 at% Ni and Cr–6 at% Ni alloys were prepared by magnetron sputtering in argon gas. The grain size of the sputtered alloys were 83 and 69 nm and in nano size. The addition of higher content of nickel reduces the grain size in the sputtered alloys. The both alloys are stable and maintain the nano-structure up to the annealing temperature of 673 K at an annealing time of 7.2 ks. Although the grain size of the alloys at a high temperature of 973 K increases on increasing the annealing time, both the alloys maintain the nano size of the grain up to an annealing time of 10 3 s. The grain size of both the alloys at 973 K definitely increases on further increasing the annealing time. Although the secondary nickel phase appears at the annealing process, the microhardness of the alloys decreases with the annealing time. The increase in grain size lowers the microhardness for the both alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Advanced Materials Characterization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (6)
Show source-provided references
1. Jose-Yacaman · Met Mater Trans · 1998 · 29A · 125
2. Roco · 2003 · 3
3. Koch · 2000 · 93
4. Mori · Proc Adv Appl Plasma Sci · 2001 · 3 · 239
5. Mori · Scr Met · 2001 · 44 · 203510.1016/S1359-6462(01)00857-0 ↗
6. B.D. Cullity, Elements of X-ray diffraction. Reading, MA: Addison-Wesley Publishers; 1956. p. 263.