Abstract
Abstract WS2/Fe/a-C/Fe multilayer films were prepared by using magnetron sputtering technique under various deposition temperatures. The composition, microstructure, mechanical and tribological properties of the films were characterized by energy dispersive spectroscopy (EDS), X-ray diffractometry (XRD), field emission scanning electron microscopy (FESEM), nano-indenter, scratch tester, film stress tester and ball-on-disk tribometer. With increasing deposition temperature, the film exhibits a morphology change from block-like to featureless, accompanied by a microstructural densification effect, its S/W ratio decreases from 1.14 to 1.04, and the hardness and adhesion are gradually enhanced. The films with deposition temperature ≥150 °C present better tribological performance than WS2/a-C multilayer film in vacuum and humid air. The film deposited at 300 °C achieves the highest hardness (9.0 GPa), a good adhesion (25.6 N), and the best tribological performance with a steady-state friction coefficient of 0.212 and wear rate of 7.07 × 10−15m3N−1m−1 in humid air, and steady-state friction coefficient of 0.165 and wear rate of 3.09 × 10−15m3N−1m−1 in vacuum.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Tribological properties of WS2 composite film prepared by a two-step method10.1016/j.vacuum.2010.03.003 ↗
2. Structure, mechanical and tribological characterisations of pulsed DC magnetron sputtered TiN-WSx composite coating10.1016/j.vacuum.2016.05.003 ↗
3. Solid lubricant coatings: recent developments and future trends10.1023/B:TRIL.0000044487.32514.1d ↗
4. Influence of substrate bias on structural and tribo-mechanical properties of pulsed magnetron sputtered TiN-WSx, hard-lubricious coating10.1016/j.triboint.2018.03.005 ↗
5. Friction behavior of pulsed Laser deposited tungsten disulfide films10.1080/10402009508983380 ↗
6. Microstructure and tribological properties of MoS2+Zr composite coatings in high humidity environment10.1016/j.apsusc.2016.01.163 ↗
7. Mechanical and tribological properties of sputter deposited nanostructured Cr-WS2 solid lubricant coatings10.1016/j.surfcoat.2010.08.074 ↗
8. Pulsed laser-ablated MoS2-Al films: friction and wear in humid conditions10.1016/j.surfcoat.2004.02.043 ↗
9. Growth, structure and friction behavior of titanium doped tungsten disulphide (Ti-WS2) nanocomposite thin films10.1016/j.tsf.2009.02.103 ↗
10. Structural, mechanical and tribological properties of WS2-Ti composite coating with and without hard under layer of TiN10.1016/j.surfcoat.2014.07.072 ↗
11. Morphology evolution of Ag alloyed WS2 films and the significantly enhanced mechanical and tribological properties10.1016/j.surfcoat.2013.10.074 ↗
12. Effect of Ag content on microstructure and tribological performance of WS2-Ag composite films10.1016/j.surfcoat.2006.02.039 ↗
13. An investigation of material and tribological properties of Sb2O3/Au-doped MoS2 solid lubricant films under sliding and rolling contact in different environments10.1016/j.surfcoat.2015.05.049 ↗
14. Environmental effects on the tribology and microstructure of MoS2-Sb2O3-C films10.1007/s11249-011-9764-z ↗
15. Extreme friction reductions during inital running-in of W-S-C-Ti low-friction coatings10.1016/j.wear.2013.01.065 ↗
16. Nanostructured WS2-Ni composite films for improved oxidation, resistance and tribological performance10.1016/j.apsusc.2013.09.024 ↗
17. Wear resistance of superior structural WS2-Sb2O3/Cu nanoscale multilayer film10.1016/j.matdes.2016.01.006 ↗
18. Rf-sputtered REMF-MoS2-Au/Au nanocomposite multilayer film10.1016/S0042-207X(01)00405-5 ↗
19. Microstructure and tribological properties of WS2/MoS2 multilayer films10.1016/j.apsusc.2011.06.148 ↗
20. Structural, morphological, chemical and tribological investigations of sputter deposited MoSx/metal multilayer coatings10.1016/S0257-8972(98)00567-2 ↗
21. Improving anti-wear and anti-corrosion properties of AM60 magnesium alloy by ion implantation and Al/AlN/CrAlN/CrN/MoS2 gradient duplex coating10.1016/j.vacuum.2013.09.002 ↗
22. Engineering applications for diamond-like carbon10.1016/0925-9635(94)90297-6 ↗
23. A long-lifetime MoS2/a-C:H nanoscale multilayer film with extremely low internal stress10.1016/j.surfcoat.2013.10.021 ↗
24. Microstructure analysis of MoS2 deposited on diamond-like carbon films for wear improvement10.1016/S0257-8972(98)00712-9 ↗
25. Instant WS2 platelets reorientation of self-adaptive WS2/a-C tribocoating10.1016/j.matlet.2018.06.111 ↗
26. Effect of carbon concentration and argon flow rate on the microstructure and triboperformance of magnetron sputtered WS2/a-C coatings10.1016/j.surfcoat.2017.06.087 ↗
27. Microstructure and tribological properties of WSx/a-C multilayer films with various layer thickness ratios in different environments10.1016/j.surfcoat.2016.11.071 ↗
28. Mechanical properties of Al/a-C nanocomposite thin films synthesized using a plasma focus device
29. Study on structure, mechanical and tribological properties of iron incorporated diamond-like carbon films10.1016/j.jnoncrysol.2016.10.018 ↗
30. The bond method used to determine the value of the lattice parameter a for α-Fe10.1002/pssa.2211210224 ↗
31. Al alloy metal matrix composites reinforced by WS2 inorganic nanomaterials10.1016/j.msea.2017.10.041 ↗
32. Comparing internal stress in diamond-like carbon films with different structure10.1016/j.tsf.2007.02.069 ↗
33. On the S/W stoichiometry and triboperformance of WSxC(H) coatings deposited by magnetron sputtering10.1016/j.surfcoat.2018.04.040 ↗
34. Reactive magnetron sputtering of tungsten disulfide (WS2-x) films: influence of deposition parameters on texture, microstructure, and stoichiometry10.1063/1.2716395 ↗
35. Deposition of c┴-oriented tungsten disulfide (WS2) films by reactive DC magnetron sputtering from a W-target in Ar/H2S10.1016/S0022-0248(97)00355-2 ↗
36. Measuring the thickness of ultra-thin diamond-like carbon films10.1016/j.carbon.2006.04.029 ↗
37. Fundamental aspects of the electronic structure, materials properties and lubrication performance of sputtered MoS2 films10.1016/0040-6090(87)90375-0 ↗
38. Effect of substrate temperature and deposition rate on the morphology and optical properties of Ti films10.1016/j.apsusc.2013.04.146 ↗
39. Theory and simulation of crystal growth10.1088/0953-8984/9/2/001 ↗
40. Enhancement of mechanical property on sputtered TiNx films with various deposition temperatures10.1166/jnn.2017.15161 ↗
41. Tribological properties of Cr- and Ti-doped MoS2 composite coatings under different humidity atmosphere10.1016/j.surfcoat.2010.06.041 ↗
42. Metal incorporation in sputter-deposited MoS2 films studied by extended x-ray absorption fine structure10.1557/JMR.1995.2091 ↗
43. Constructing WS2/MoS2 nano-scale multilayer film and understanding its positive response to space environment10.1016/j.surfcoat.2018.08.072 ↗
44. Model of superlattice yield stress and hardness enhancements10.1063/1.359467 ↗
45. Hardness and stability of metal-nitride nanoscale multilayers10.1016/j.scriptamat.2003.11.042 ↗
46. Residual stresses in evaporated silicon dioxide thin films: correlation with deposition parameters and aging behavior10.1063/1.360290 ↗
47. Sputtering deposited TiNi films: relationship among processing, stress evolution and phase transformation behaviors10.1016/S0257-8972(02)00896-4 ↗
48. Finite element simulation of residual stress of double-ceramic-layer La2Zr2O7/8YSZ thermal barrier coatings using birth and death element technique10.1016/j.commatsci.2011.09.028 ↗
49. Deposition stress effects on the life of thermal barrier coatings on burner rigs10.1016/0040-6090(84)90533-9 ↗