Interfacial microstructure and mechanical properties of the TiC-Ni cermet/Ag-Cu-Zn/Invar joint

Min Lei, Yulong Li, Hua Zhang

Vacuum· Volume 168
Publisher page

Abstract

Abstract TiC-Ni cermet and Invar was brazed with Ag-Cu-Zn alloy in vacuum and the interfacial microstructure and mechanical properties were studied. The interfacial microstructure of the joint brazed at 910 °C for 10 min was TiC-Ni cermet/(Ag) + (Cu, Ni) + TiC/(Cu, Ni) + (Ag)/(Cu, Ni)/(Cu, Ni) + (Fe, Ni)/Invar alloy. When the temperature increased from 740 °C to 940 °C, (Cu, Ni) reactive layer at the cermet side dissolved into the brazing seam and became discontinuous. Moreover, TiC particles presented gradient distribution in the reactive region of the joint brazed between 850 °C and 940 °C. Meanwhile, the amount of (Cu, Ni) detaching from the cermet and entering the brazing seam increased. The shear strength firstly increased and then sharply decreased with temperature. The maximum shear strength of 161 MPa was obtained at 910 °C for 10 min and the joint was fractured on (Ag). The change trend of the shear strength between 820 °C and 940 °C was attributed to the increase thickness of the functional gradient material layer in the reactive region and the decrease of the (Cu, Ni) amount in the penetration region and the reactive region with the temperature increase.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Additional active metal Nb in Cu-Ni system filler metal for brazing of TiC cermet/steel10.1016/j.matlet.2015.04.126 ↗
2. 3D gel printing of graded TiC-high manganese steel cermet10.1007/s10853-018-2945-5 ↗
3. Quantitative research on microstructure and thermal physical mechanism in laser melting deposition for Invar alloy10.1016/j.jmapro.2017.11.018 ↗
4. Relief of the residual stresses in Si3N4/Invar joints by multi-layered braze structure-Experiments and simulation10.1016/j.ceramint.2016.01.096 ↗
5. Microstructure and mechanical properties of invar alloy and Si3N4 ceramic brazed joints
6. Enhanced strength and fatigue life of ultra-fine grain Fe-36Ni Invar alloy10.1016/S0921-5093(03)00082-0 ↗
7. Interface structure and mechanical properties of the brazed joint of TiC cermet and steel10.1016/j.jeurceramsoc.2005.01.043 ↗
8. Brazing temperature and time effects on the mechanical properties of TiC cermet/Ag-Cu-Zn/steel joints10.1016/j.msea.2005.11.044 ↗
9. Interface structure and mechanical properties of Ti(C,N)-based cermet and 17-4PH stainless steel joint brazed with nickel-base filler metal BNi-210.1016/j.jmatprotec.2011.06.003 ↗
10. Interfacial microstructure and mechanical properties of TZM alloy and ZrC particle reinforced tungsten composite joint brazed using Ti-61Ni filler10.1016/j.jallcom.2018.02.258 ↗
11. Ni-Cu alloy for diffusion bonding cermet/steel in air10.1016/j.matlet.2009.06.042 ↗
12. Characterization of Al/Ni multilayers and their application in diffusion bonding of TiAl to TiC cermet10.1016/j.tsf.2012.01.001 ↗
13. Investigation of joining Al-C-Ti cermets and Ti6Al4V by combustion synthesis10.1016/j.mseb.2011.12.041 ↗
14. Microstructure evolution and reaction mechanism during reactive joining of TiAl intermetallic to TiC cermet using Ti-Al-C-Ni interlayer10.1016/j.jallcom.2006.07.040 ↗
15. Metallurgical and electrochemical characterization of contemporary silver-based soldering alloys10.2319/073013-569.1 ↗
16. Influence of sulphur on the microstructure and properties of Ag-Cu-Zn brazing filler metal10.1179/1743284713Y.0000000284 ↗
17. Study on microstructure and property of brazed joint of AgCuZn-X(Ga, Sn, In, Ni) brazing alloy10.1016/S1875-5372(10)60087-2 ↗
18. Weld metal composition change during conduction mode laser welding of aluminum alloy 518210.1007/s11663-001-0018-6 ↗
19. Effect of calcium on the microstructure and mechanical properties of brazed joint using Ag-Cu-Zn brazing filler metal10.1016/j.matdes.2012.11.021 ↗
20. In situ synthesis of high strength Ag brazing filler metals during induction brazing process10.1016/j.scriptamat.2015.07.041 ↗
21. Effect of silver content on microstructure and properties of brass/steel induction brazing joint using Ag-Cu-Zn-Sn filler metal10.1016/S1005-0302(11)60077-7 ↗
22. Effect of AgCuZnCd solder on the wettability of stainless steel braze welding
23. Vacuum brazing TiAl-based alloy to 40Cr steel using Ag-Cu-Zn filler metal10.1023/A:1014269923133 ↗
24. Microstructure and shear strength of the brazed joint of Ti(C,N)-based cermet to steel10.1007/s12598-010-0013-7 ↗
25. Diffusion brazing of Ti-6Al-4V and austenitic stainless steel using silver-based interlayer10.1016/j.matdes.2013.07.103 ↗
26. Brazing of stainless steels using Cu-Ag-Mn-Zn braze filler: studies on wettability, mechanical properties, and microstructural aspects10.1016/j.matdes.2017.02.057 ↗
27. Reactive wetting of TiC-Ni cermet by Ag-Cu-Zn alloy during evaporation10.1016/j.vacuum.2017.01.014 ↗
28. Joining of SiO2 ceramic and TC4 alloy by nanoparticles modified brazing filler metal
29. Microstructures of eutectic and near eutectic specimens in the ternary AgCuZn system10.1179/cmq.1980.19.4.345 ↗
30. Constitution and properties of some iron-bearing cupro-nickels10.1007/BF03397649 ↗
31. Phase equilibria of the ternary Ag-Cu-Ni system and the interfacial reactions in the Ag-Cu/Ni couples10.1007/BF00355906 ↗
32. Reactive wetting in titanium carbide/non-reactive metal systems10.1016/j.cossms.2006.02.008 ↗
33. Wetting of carbide ceramics (B4C, SiC, TiC and ZrC) by molten Ni at 1753 K10.1016/j.jallcom.2015.07.138 ↗
34. Theoretical calculations of the surface tension of Ag(1-x)-Cu(x) liquid alloys10.1016/j.jallcom.2011.02.148 ↗
35. Interlayer of Al2O3-Cr functionally graded material for reduction of thermal stresses in alumina-heat resisting steel joints10.1016/j.jeurceramsoc.2006.04.102 ↗