Abstract

Abstract The present work studied the fracture behaviour of a brittle film/ductile substrate under a sphero-conical indenter. To understand the effect of film thickness, the amorphous carbon films were prepared with different thicknesses, i.e. 140 nm, 400 nm and 1300 nm, on a poly-ether-ether-ketone substrate. It was found that multiple ring-like cracks occur for all the films under nanoindentations. However, film spalling between ring cracks was noticed for the film with 1300 nm thickness; whereas spalling was observed at the center of indent for the thin film with the thickness of 140 nm. Finite element analysis revealed that different crack patterns were resulted from different stress distributions in the film-substrate systems, depending on the film thickness. In particular, when the film is thick the cracks were mostly caused by the contact stress induced by the indenter. For a thin film, however, the ring cracks could be formed due to the bending stress caused by the plastic zone in the substrate. Moreover, a dimensional analysis was preformed to quantitatively determine the ratio of bending stress and contact stress in different brittle film/ductile substrate system. The new findings of the thickness effect are important for fracture analysis of brittle films using nanoindentations.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Gradient DLC-based nanocomposite coatings as a solution to improve tribological performance of aluminum alloy10.1007/s11249-010-9585-5 ↗
2. The cracking and decohesion of thin films on ductile substrates10.1016/0001-6160(89)90018-7 ↗
3. Erosion resistance of the nanostructured Cr/CrN multilayer coatings on Ti6Al4V alloy10.1016/j.vacuum.2014.02.024 ↗
4. Analysis on multiple ring-like cracks in thin amorphous carbon film on soft substrate under nanoindentation10.1088/0022-3727/46/50/505314 ↗
5. Fracture mechanisms of thin amorphous carbon films in nanoindentation10.1016/S1359-6454(97)00143-2 ↗
6. Indentation stress-based models to predict fracture properties of brittle thin film on a ductile substrate10.1016/j.surfcoat.2016.03.067 ↗
7. Microstructure development and properties of the AlCuFe quasicrystalline coating on near-α titanium alloy10.1016/j.apsusc.2011.09.013 ↗
8. An energy method to analyze through thickness thin film fracture during indentation10.1016/j.tsf.2006.01.043 ↗
9. Toughness measurement of thin films based on circumferential cracks induced at conical indentation10.1007/s10704-015-0022-5 ↗
10. Analysis on spiral crack in thick diamond-like carbon film subjected to spherical contact loading10.1016/j.msea.2008.04.069 ↗
11. Three-dimensional study of indentation-induced cracks in an amorphous carbon coating on a steel substrate10.1557/jmr.2006.0313 ↗
12. Indentation fracture and toughness assessment for thin optical coatings on glass10.1088/0022-3727/40/18/S01 ↗
13. Analysis on cracking in hard thin films on a soft substrate under Berkovich indentation10.1016/j.vacuum.2014.11.013 ↗
14. Analysis methods and size effects in the indentation fracture toughness assessment of very thin oxide coatings on glass10.1016/j.crme.2011.05.009 ↗
15. Probing mechanical properties of thin film and ceramic materials in micro-and nano-scale using indentation techniques10.1016/j.apsusc.2010.06.006 ↗
16. Properties of nanocrystalline Al–Cu–O films reactively sputtered by DC pulse dual magnetron10.1016/j.apsusc.2011.10.039 ↗
17. Microstructure, residual stress, and fracture of sputtered TiN films10.1016/j.surfcoat.2013.03.009 ↗
18. Measurement of fracture toughness of ultra-thin amorphous carbon films10.1016/S0040-6090(97)00788-8 ↗
19. Atomic layer deposition of Al2O3 and Al2O3/TiO2 barrier coatings to reduce the water vapour permeability of polyetheretherketone10.1016/j.tsf.2015.08.038 ↗
20. Numerical estimation of fracture toughness from indentation-induced circumferential cracking in thin films on ductile substrates10.1016/j.ijsolstr.2013.06.009 ↗
21. Nanoindentation-induced interfacial fracture of ZnO thin films deposited on Si (111) substrates by atomic layer deposition10.1016/j.jallcom.2013.10.213 ↗
22. Analysis of spherical indentations of coating-substrate systems: experiments and finite element modeling10.1016/j.matdes.2012.06.040 ↗
23. Plasma polymer surfaces compatible with a CMOS process for direct covalent enzyme immobilization10.1002/ppap.200800108 ↗
24. Comparison on protein adsorption properties of diamond-like carbon and nitrogen-containing plasma polymer surfaces10.1016/j.tsf.2011.11.054 ↗
25. Mechanical behaviour characterisation of silicon and effect of loading rate on pop-in: a nanoindentation study under ultra-low loads10.1016/j.msea.2008.11.021 ↗
26. Determination of plastic properties of metals by instrumented indentation using different sharp indenters10.1016/S1359-6454(02)00568-2 ↗
27. Tensile strength of DLC films evaluated by a nanomaterials testing system10.1016/j.diamond.2012.01.027 ↗
28. A superhard diamond-like carbon film10.1016/S0925-9635(99)00344-1 ↗
29. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
30. Fracture analysis of diamond-like carbon films under conical nanoindentation