Growth defects in magnetron sputtered PVD films deposited in UHV environment
Source abstract
Abstract
The growth defects in magnetron sputtered coatings have been well studied in industrial environment. In this work, on the other hand, the emphasis is in observing the same phenomena in a lab-scale UHV environment. TiN and CrN films were deposited at a thickness of 1-2 mu m. The statistical evaluation of defect density was based on stylus profilometry scans (2 mm(2) area), and consequent analysis of hillock density in dependence of threshold height. Morphology of defects was observed by SEM, while on selected defects we made FIB cross-sections. In this way we were able to measure the chemical composition of individual seeds - starting points for growth defects. In contrast to expectations, there was only a relatively minor reduction of defect density by using UHV environment. (C) 2016 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Plasma Diagnostics and Applications · Advanced Sensor Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. Corrosion protection with hard coatings on steel: past approaches and current research efforts10.1016/j.surfcoat.2014.08.069 ↗
2. Identification of the growth defects responsible for pitting corrosion on sputter-coated steel samples by large area high resolution mapping10.1016/j.tsf.2014.12.014 ↗
3. Tribological and corrosion behavior of CrN coatings: roles of substrate and deposition defects10.1016/j.surfcoat.2014.07.063 ↗
4. The role of surface defects density on corrosion resistance of PVD hard coatings10.1002/ppap.200731416 ↗
5. Growth defect density in PVD hard coatings prepared by different deposition techniques10.1016/j.surfcoat.2013.09.020 ↗
6. SEM study of defects in PVD hard coatings10.1016/j.vacuum.2007.07.005 ↗
7. Growth defects in PVD hard coatings10.1016/j.vacuum.2009.05.018 ↗
8. Growth effects in carbon coatings deposited by magnetron sputtering10.1016/S0257-8972(03)00010-0 ↗
9. Factors affecting growth defect formation in cathodic arc evaporated coatings10.1016/0257-8972(95)02773-4 ↗
10. Fine particles in dusty plasmas10.1016/S0042-207X(02)00132-X ↗
11. Surface density of growth defects in different PVD hard coatings prepared by sputtering10.1016/j.vacuum.2011.07.013 ↗
12. K. Salamon, N. Radić, I. Bogdanović Radović, M. Očko, Phase map, composition and resistivity of reactively magnetron sputtered and annealed Ta–N films.
13. SEM study of defects in PVD hard coatings using focused ion beam milling10.1016/j.surfcoat.2007.09.033 ↗