journal article·2016-07

Effect of anodizing temperature on surface morphology evolution of sputtered hematite films: A potential post-treatment method for further photoelectrochemical performance enhancement

Mao-Chia Huang, TsingHai Wang, Wen-Sheng Chang, Ching-Chen Wu, Jing-Chie Lin, Cheng-Hsueh Lee, Shih-Hsuan Huang

Vacuum· Volume 129
Publisher page

Abstract

Abstract In this study, effect of anodization temperature on the photoelectrochemical (PEC) performance of nanostructured hematite films prepared by anodizing the sputtered iron films on the fluorine-doped SnO 2 glass substrate was investigated. It was noted that increasing the anodization temperature would induce the hematite nanostructure developing from film-like to nanorod morphology. Importantly, this morphology transformation is noted to accompany with the enhanced PEC performance up to 0.59 mA/cm 2 (nanorod structured anodized at 60 °C). Our results clearly demonstrated that the potential of post-treatment using anodization to further enhance the PEC performance of hematite films.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Iron oxide chemistry and applications · Advanced Photocatalysis Techniques · Copper-based nanomaterials and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Fujishima · Nature · 1972 · 238 · 3710.1038/238037a0 ↗
2. Lai · J. Alloys Compd. · 2013 · 547 · 4310.1016/j.jallcom.2012.08.121 ↗
3. Abe · ChemSusChem · 2011 · 4 · 22810.1002/cssc.201190005 ↗
4. Shangguan · RSC Adv. · 2013 · 3 · 1016310.1039/c3ra41439f ↗
5. Chen · Small · 2013 · 9 · 292610.1002/smll.201202547 ↗
6. Shibli · RSC Adv. · 2015 · 5 · 1939310.1039/C4RA12646G ↗
7. Yehezkeli · RSC Adv. · 2015 · 5 · 5875510.1039/C5RA10454H ↗
8. Cao · Vacuum · 2014 · 102 · 110.1016/j.vacuum.2013.10.025 ↗
9. Deng · Surf. Coat. Technol. · 2015 · 266 · 18310.1016/j.surfcoat.2015.02.042 ↗
10. Huang · J. Alloys Compd. · 2015 · 636 · 17610.1016/j.jallcom.2015.02.166 ↗
11. Ling · Nano Lett. · 2011 · 11 · 211910.1021/nl200708y ↗
12. Huang · Appl. Surf. Sci. · 2014 · 301 · 36910.1016/j.apsusc.2014.02.085 ↗
13. Huang · Nanosci. Nanotechnol. Lett. · 2015 · 7 · 29710.1166/nnl.2015.1915 ↗
14. Murphy · Int. J. Hydrogen Energy · 2006 · 31 · 199910.1016/j.ijhydene.2006.01.014 ↗
15. Kleiman-Shwarsctein · J. Phys. Chem. C · 2008 · 112 · 1590010.1021/jp803775j ↗
16. Huang · Ceram. Int. · 2014 · 40 · 1053710.1016/j.ceramint.2014.03.029 ↗
17. Mohapatra · Chem. Mater. · 2009 · 21 · 304810.1021/cm8030208 ↗
18. Rangaraju · J. Phys. D. Appl. Phys. · 2009 · 42 · 13530310.1088/0022-3727/42/13/135303 ↗
19. Chang · Int. J. Hydrogen Energy · 2012 · 37 · 1361610.1016/j.ijhydene.2012.01.136 ↗
20. Wu · Nano Lett. · 2014 · 14 · 600210.1021/nl503059t ↗
21. Wang · Electrochim. Acta · 2013 · 28 · 307
22. Zhang · Vacuum · 2014 · 99 · 16010.1016/j.vacuum.2013.05.019 ↗
23. Huang · Appl. Surf. Sci. · 2016 · 360 · 44210.1016/j.apsusc.2015.09.174 ↗
24. Wang · J. Phys. Chem. C · 2009 · 113 · 402610.1021/jp811201x ↗
25. Qian · Adv. Mater. · 2009 · 21 · 366310.1002/adma.200900525 ↗
26. Yu · Environ. Sci. Technol. · 2008 · 42 · 490210.1021/es800036n ↗
27. Osterloh · Chem. Soc. Rev. · 2013 · 42 · 229410.1039/C2CS35266D ↗
28. McDonald · Chem. Mater. · 2011 · 23 · 168610.1021/cm1020614 ↗
29. Klahr · J. Am. Chem. Soc. · 2012 · 134 · 1669310.1021/ja306427f ↗
30. Barroso · J. Am. Chem. Soc. · 2011 · 133 · 1486810.1021/ja205325v ↗
31. Huang · J. Alloys Compd. · 2014 · 606 · 18910.1016/j.jallcom.2014.04.001 ↗
32. Kment · ACS Nano · 2015 · 9 · 711310.1021/acsnano.5b01740 ↗