journal article·2011-01

Effect of temperature on microstructure and electrical properties of TaSi2 thin films grown on Si substrates

A.N. Mansour

Vacuum· Volume 85· Issue 6
Publisher page

Abstract

Abstract Tantalum silicide (TaSi 2 ) thin films were deposited on n-type silicon single crystal substrates using a dual electron-gun system and with Ta and Si targets. The thicknesses of TaSi 2 thin films considered in this study are in the range 200–500 nm, respectively. The TaSi 2 /Si samples were annealed at temperature 1173 K for 2 h in a vacuum of 10 −8 mbar. The structure of the tantalum silicide thin films was investigated by X-ray diffraction (XRD). X-ray diffraction results show changes in the structure of TaSi 2 thin films from amorphous to crystalline after annealing. According to XRD analysis, a complete conversion to single-phase disilicide TaSi 2 was achieved from a sample composition of Ta:Si = 1:2. DC conductivity was measured for the TaSi 2 thin films in the temperature range 300–900 K before and after annealing. It has been observed that the DC conductivity and activation energy was affected by changing the TaSi 2 film thickness and by annealing. The experimental results indicate that, the conduction phenomena of the investigated sample proceeded via two distinct mechanisms. The first one in the low-temperature range T 4 Ω −1 cm −1 . The other process appears in the high temperature region T > 500 K, where thermally activated conduction occurs through the extended states. Here the value of the pre-exponential factor before and after annealing is larger than 10 4 Ω −1 cm −1 . The conductivity is greater in the crystalline phase than in the amorphous phase. The activation energy Δ E for our films before and after annealing is increased with increasing film thickness.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and interfaces · Silicon Nanostructures and Photoluminescence · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Murarka · 1983
2. Mohammadi · Solid State Technol · 1981 · 24 · 65
3. Sinha · 1982 · 173
4. Nicolet · 1983 · vol. 6
5. Bucher · 1984
6. Ino · Jap J Appl Phys · 1998 · 37 · 427710.1143/JJAP.37.4277 ↗
7. Cho · Thin Soild Films · 1992 · 221 · 20310.1016/0040-6090(92)90815-S ↗
8. Wetzig · 2003
9. Murarka · J Appl Phys · 1980 · 51 · 35010.1063/1.327379 ↗
10. Yanagisawa · J Electrochem Soc · 1980 · 127 · 112010.1149/1.2129830 ↗
11. Christou · J Electron Mater · 1976 · 5 · 110.1007/BF02652882 ↗
12. Revesz · J Electrochem Soc · 1976 · 123 · 151410.1149/1.2132629 ↗
13. Muraraka · J Appl Phys · 1980 · 51 · 159310.1063/1.327814 ↗
14. A comparative study on combustion synthesis of Ta–Si compounds10.1016/j.intermet.2007.03.004 ↗
15. A.N. Mansour, 1988. Suez Canal University, Egypt, Ph.D. thesis.
16. Natan · Mater Lett · 1985 · 3 · 810.1016/0167-577X(85)90031-X ↗
17. Cho · Appl Phys Com · 1992 · 11 · 127
18. Kwak · J Appl Phys · 1999 · V8510.1063/1.370209 ↗
19. Standard Diffraction Powder Pattern No. 8–53.
20. Abu-Sehly · J Mater Sci · 2000 · 35 · 200910.1023/A:1004791124418 ↗
21. Abu-Sehly · J Phys Chem Sol · 2001 · 36 · 136
22. Mott · Philos Mag · 1970 · 22 · 710.1080/14786437008228147 ↗
23. Mott · Philos Mag · 1970 · 22 · 90310.1080/14786437008228147 ↗
24. H.A. Zayed and A. Fizika, 1995. 4, 45.
25. Lyubin · Fizika Tverdogo Tela · 1964 · 6 · 3740
26. El-Mandouh · J Appl Phys · 1995 · 78 · 715610.1063/1.360424 ↗