journal article·2020-03

Long-term stability and disappearing anode effects during reactive DC and pulsed bipolar magnetron sputtering of Al2O3

Pavel Mareš, Stanislav Kadlec, Martin Dubau, Aleš Marek, Jiří Vyskočil

Vacuum· Volume 173
Publisher page

Abstract

Abstract Reactive magnetron sputtering is a well-established technique to deposit compound films with different composition. Target poisoning influences the process stability and gives rise to hysteresis effects. Recently, a double S-shaped hysteresis curve has been reported, meaning two values of discharge voltage correspond to one defined value of the reactive gas partial pressure. In the present study, the long-term stability of the hysteresis behavior was studied in an industrial system equipped with a mass spectrometer, an optical emission spectrometer and an external anode. Cycles of decreasing and increasing the target voltage have been repeated several times for single Al alloy target DC sputtering and bipolar pulsed sputtering. In the first case, changes in the hysteresis S-shaped curve depending on time were detected indicating that the system moves towards the poisoned mode meaning higher currents at low voltages and vice versa. When an external additional anode is opened, the system instantly reacts by moving closer to the metallic mode. All of our observations indicate that the long-term behavior is caused by the effect of a disappearing anode and corresponding effects on the plasma medium. Bipolar sputtering reduces considerably the effects of disappearing anode, but a long time evolution can still be seen.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Semiconductor materials and devices · Ion-surface interactions and analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Very-high-rate reactive sputtering of alumina hard coatings10.1016/S0257-8972(97)00152-7 ↗
2. Relation of hardness and oxygen flow of Al2O3 coatings deposited by reactive bipolar pulsed magnetron sputtering10.1016/j.tsf.2005.08.162 ↗
3. Comparative characterization of alumina coatings deposited by RF, DC and pulsed reactive magnetron sputtering10.1016/S0257-8972(99)00458-2 ↗
4. An Al2O3 sensor for low humidity content: characterization by impedance spectroscopy10.1016/0925-4005(96)80100-6 ↗
5. Main properties of Al2O3 thin films deposited by magnetron sputtering of an Al2O3 ceramic target at different radio-frequency power and argon pressure and their passivation effect on p-type c-Si wafers10.1016/j.tsf.2016.10.049 ↗
6. Thermal stability of alumina thin films containing γ-Al2O3 phase prepared by reactive magnetron sputtering10.1016/j.apsusc.2010.07.107 ↗
7. Reactive d.c. magnetron sputter deposited Al2O3 films: large-area coatings for industrial applications10.1016/S0257-8972(99)00378-3 ↗
8. Low-temperature deposition of nanocrystalline Al2O3 films by ion source-assisted magnetron sputtering10.1016/j.vacuum.2018.01.009 ↗
9. Effect of bias voltage on microstructure and optical properties of Al2O3 thin films prepared by twin targets reactive high power impulse magnetron sputtering10.1016/j.vacuum.2019.04.060 ↗
10. Review Article: tracing the recorded history of thin-film sputter deposition: from the 1800s to 201710.1116/1.4998940 ↗
11. Recent aspects concerning DC reactive magnetron sputtering of thin films: a review10.1016/S0257-8972(00)00566-1 ↗
12. Process modeling of reactive sputtering10.1116/1.576259 ↗
13. Return of target material ions leads to a reduced hysteresis in reactive high power impulse magnetron sputtering: Experiment10.1063/1.4977816 ↗
14. Return of target material ions leads to a reduced hysteresis in reactive high power impulse magnetron sputtering: Model10.1063/1.4977815 ↗
15. Tutorial: reactive high power impulse magnetron sputtering (R-HiPIMS)10.1063/1.4978350 ↗
16. Hysteresis effect in reactive sputtering: a problem of system stability10.1088/0022-3727/19/9/004 ↗
17. Reactive magnetron sputtering of thin films: present status and trends10.1016/j.tsf.2004.07.041 ↗
18. Control of reactive sputtering processes10.1016/j.tsf.2005.05.022 ↗
19. Process stabilization and a significant enhancement of the deposition rate in reactive high-power impulse magnetron sputtering of ZrO2 and Ta2O5 films10.1016/j.surfcoat.2013.10.052 ↗
20. Mechanisms of voltage controlled, reactive, planar magnetron sputtering of Al in Ar/N2 and Ar/O2 atmospheres10.1116/1.572395 ↗
21. Voltage controlled reactive sputtering process for aluminium oxide thin films10.1016/S0040-6090(98)00546-X ↗
22. High rate deposition of Al2O3 coatings reactively sputter deposited10.1002/ppap.200730606 ↗
23. The problem of reactive sputtering and cosputtering of elemental targets10.1016/0040-6090(82)90162-6 ↗
24. The existence of a double S-shaped process curve during reactive magnetron sputtering10.1063/1.4962958 ↗
25. Reactive sputtering of metal targets: influence of reactive atoms implantation
26. Hysteresis and process stability in reactive high power impulse magnetron sputtering of metal oxides10.1016/j.tsf.2011.06.021 ↗
27. Aspects and results of long-term stable deposition of Al2O3 with high rate pulsed reactive magnetron sputtering10.1016/0257-8972(93)90079-4 ↗
28. Ensuring long-term stability of process and film parameters during target lifetime in reactive magnetron sputtering10.1016/S0257-8972(01)01507-9 ↗
29. DC reactive magnetron sputtering with Ar ion-beam assistance for titanium oxide films10.1016/S0257-8972(02)00286-4 ↗
30. Redundant anode sputtering: a novel approach to the disappearing anode problem
31. Reactive sputtering using a dual-anode magnetron system, Society of Vacuum coaters
32. Mid-frequency sputtering of dielectrics: Al2O310.1016/S0257-8972(03)00369-4 ↗
33. Dual-anode magnetron sputtering10.1016/S0257-8972(02)00659-X ↗
34. The disappearing anode myth: strategies and solutions for reactive PVD from single magnetrons10.1016/S0257-8972(97)00438-6 ↗
35. Discharge voltage measurements during magnetron sputtering10.1016/j.surfcoat.2005.02.166 ↗
36. Ion secondary electron emission from Al2O3 and MgO films10.1016/0038-1098(86)90266-8 ↗
37. Pulsed magnetron sputtering – process overview and applications