Effect of SiC nanoparticle concentration on the properties of oxide films formed on Ti–10V–2Fe–3Al alloy
Source abstract
Abstract
Abstract Ordinary and composite oxide films were formed on Ti–10V–2Fe–3Al alloy by anodic oxidation process, in the environmentally friendly electrolytes with different concentrations of SiC nanoparticle. The surface morphology and phase compositions of the oxide film were analyzed by field emission scanning electron microscopy and Raman spectrum techniques, respectively. The results showed that the oxide film was covered with rod–like and rimose protuberances, being mainly composed of anatase, rutile, vanadium pentoxide, aluminum oxide and ferric oxide. The thickness was determined by SEM, increasing with a corresponding increase of SiC nanoparticle concentration. The wear resistance and corrosion resistance of the oxide films were evaluated by the ball–on–disc rotating wear tester and potentiodynamic polarization tests at room temperature, respectively. It was found that composite films possessed enhanced wear resistance and corrosion resistance comparing with the ordinary film. However, the wear resistance of oxide film was not better with higher concentration of SiC nanoparticle. The optimal concentrations of nanoparticle aiming at excellent wear resistance and corrosion resistance were 5 and 10 g/L, respectively. The friction coefficient and wear weight loss were 0.18 and 4.2 mg; the corrosion potential and corrosion current density were 0.665 V and 3.65 × 10−10 A/cm2.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Characterization of titanium alloy Ti–6Al–4V for chemical, marine and industrial applications10.1016/j.matchar.2003.10.006 ↗
2. A comparison of corrosion, tribocorrosion and electrochemical impedance properties of pure Ti and Ti6Al4V alloy treated by micro-arc oxidation process10.1016/j.apsusc.2014.11.030 ↗
3. Time dependence of microstructure and hardness in plasma carbonized Ti–6Al–4V alloys10.1016/j.vacuum.2013.02.004 ↗
4. Tribological properties of titanium alloys10.1016/0043-1648(91)90249-T ↗
5. Study plasma electrolytic oxidation process and characterization of coatings formed in an alumina nanoparticle suspension10.1016/j.vacuum.2014.05.008 ↗
6. Abrasive wear behaviour of Si3N4/TiO2 nanocomposite coatings fabricated by plasma electrolytic oxidation10.1016/j.surfcoat.2010.03.052 ↗
7. Corrosion–resistant composite titanium nitride layers produced on the AZ91D magnesium alloy by a hybrid method10.1016/j.vacuum.2013.06.018 ↗
8. AC plasma electrolytic oxidation of magnesium with zirconia nanoparticles10.1016/j.apsusc.2008.04.100 ↗
9. Tribological characterization of microarc oxidized alumina coatings for biological applications10.1016/j.vacuum.2008.03.085 ↗
10. Corrosion resistance of the surface layers formed on titanium by plasma electrolytic oxidation and hydrothermal treatment10.1016/j.vacuum.2005.01.017 ↗
11. Electrophoretic deposition of PTFE particles on porous anodic aluminum oxide film and its tribological properties10.1016/j.apsusc.2013.11.114 ↗
12. One–step preparation of TiO2/MoS2 composite coating on Ti6Al4V alloy by plasma electrolytic oxidation and its tribological properties10.1016/j.surfcoat.2012.10.079 ↗
13. Pulse electrodeposition of Ni–P matrix composite coatings reinforced by SiC particles10.1016/j.jallcom.2010.01.057 ↗
14. Microstructure and microhardness of SiC nanoparticles reinforced magnesium composites fabricated by ultrasonic method10.1016/S0921-5093(04)00936-0 ↗
15. Effect of SiC particle impact nano–texturing on tribological performance of 304L stainless steel10.1016/j.apsusc.2014.06.173 ↗
16. Corrosion protection and formation mechanism of anodic coating on SiCp/Al metal matrix composite10.1016/j.tsf.2011.01.030 ↗
17. Composite Electrodeposition to Obtain Nanostructured Coatings10.1149/1.1377279 ↗
18. The effects of spark anodizing treatment of pure titanium metals and titanium alloys on corrosion characteristics10.1016/j.surfcoat.2006.11.022 ↗
19. Synthesis of a porous oxide layer on a multifunctional biomedical titanium by micro-arc oxidation10.1016/j.msec.2009.03.004 ↗
20. The tribology properties of alumina/silica composite nanoparticles as lubricant additives10.1016/j.apsusc.2011.01.084 ↗
21. Effect of hydrostatic pressure on the Raman spectrum of anatase (TiO2)10.1016/0038-1098(79)90648-3 ↗
22. In situ IR, Raman, and UV–Vis DRS spectroscopy of supported vanadium oxide catalysts during methanol oxidation10.1023/A:1027275225668 ↗
23. Effects of hyperthermia induced crystalline aggregation on properties of TiO2 thin films10.1179/1743294414Y.0000000286 ↗
24. Evaluation of corrosion and tribocorrosion of plasma electrolytic oxidation treated Ti–6Al–4V alloy10.1016/j.surfcoat.2014.01.042 ↗
25. XPS study on Al2O3– and AlPO4–Coated LiCoO2 cathode material for high–capacity Li ion batteries10.1149/1.2789299 ↗
26. Analysis of XPS spectra of double layer films of Fe2O3/SnO2 and SnO2/Fe2O3
27. Effect of the thickness of cold sprayed aluminium alloy coating on the adhesive bond strength with an aluminium alloy substrate10.1016/j.surfcoat.2015.02.048 ↗
28. Structure and property of anodic oxide films enhanced by SiC nanoparticles on aluminum alloy
29. Study on corrosion resistance and roughness of micro-plasma oxidation ceramic coatings on Ti alloy by EIS technique10.1016/j.electacta.2006.12.052 ↗
30. Effect of alumina sol addition to micro-arc oxidation electrolyte on the properties of MAO coatings formed on magnesium alloy AZ91D10.1016/j.jallcom.2010.02.098 ↗
31. Growth of ceramic coatings on AZ91D magnesium alloys by micro-arc oxidation in aluminate–fluoride solutions and evaluation of corrosion resistance10.1016/j.apsusc.2004.11.031 ↗