Abstract
Abstract In order to investigate the effect of the evaporation on wetting, reactive wetting of TiC-Ni cermet by molten Ag-Cu-Zn alloys with different Zn contents was studied at 810 °C using a sessile drop method in vacuum. The vapor recoil force induced by the strong evaporation of Zn in the Ag-Cu-25Zn alloy drove the spreading of the molten Ag-Cu-25Zn alloy. Furthermore, the sequential evaporation of Zn in the Ag-Cu-25Zn alloy caused the formation of a (Cu, Ni) solid-solution layer at the interface between the TiC-Ni cermet and the Ag-Cu-Zn alloy. Thus, the (Cu, Ni) solid-solution layer could serve as a metallization layer on the surface of the TiC-Ni cermet, which promoted the non-wetting to wetting transition of the TiC-Ni cermet by the Ag-Cu-25Zn alloy. The equilibrium contact angle of the Ag-Cu-25Zn alloy on the TiC-Ni cermet was 19.9°, approximately equal to that of a Ag-28Cu eutectic alloy on a Cu-Ni alloy surface. The final contact angle of the Ag-Cu-Zn liquid alloy on the TiC-Ni cermet first decreased and then increased as the Zn content in the liquid was increased from 0% to 30%. It reached a minimum value in the Ag-Cu-25Zn alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Electronic Packaging and Soldering Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Effects of Cu interlayer on the wettability of aluminum on carbon10.1016/j.jallcom.2013.05.190 ↗
2. Plasma treatment on SiO2f/SiO2 composites for their assisted brazing with Nb10.1016/j.vacuum.2015.10.025 ↗
3. Progress in understanding and modeling reactive wetting of metals on ceramics10.1016/j.cossms.2006.04.004 ↗
4. Enhanced wetting of dual-phase metallic solids by liquid metals: a new effect of interfacial reaction10.1016/j.actamat.2013.03.039 ↗
5. Reactive wetting of AgCuTi filler metal on the TiAl-based alloy substrate10.1016/j.apsusc.2012.07.047 ↗
6. Evaluation of unusual change in contact angle between MgO and molten magnesium10.1016/j.msea.2005.10.055 ↗
7. Wetting of polycrystalline MgO by molten Mg under evaporation10.1016/j.matchemphys.2010.02.052 ↗
8. Wettability of pure Ti by molten pure Mg droplets10.1016/j.actamat.2009.09.039 ↗
9. Pinning-depinning behavior in the wetting of (0001) α-Al2O3 single crystal by molten Mg10.1016/j.apsusc.2011.07.090 ↗
10. Wetting and evaporation behaviors of molten Mg-Al alloy drops on partially oxidized α-SiC substrates10.1016/j.matchemphys.2011.08.051 ↗
11. Wetting of (0001) α-alumina single crystals by molten Mg–Al alloys in the presence of evaporation10.1007/s10853-012-6784-5 ↗
12. Weld metal composition change during conduction mode laser welding of aluminum alloy 518210.1007/s11663-001-0018-6 ↗
13. The hydrodynamic stability of rapidly evaporating liquids at reduced pressure10.1017/S0022112076000347 ↗
14. The spreading of volatile liquid droplets on heated surfaces10.1063/1.868623 ↗
15. Voltage-induced spreading and superspreading of liquids10.1038/ncomms2619 ↗
16. Brazing temperature and time effects on the mechanical properties of TiC cermet/Ag-Cu-Zn/steel joints10.1016/j.msea.2005.11.044 ↗
17. Microstructure and mechanical properties of TiC-WC-(Ti, W)C-Ni cermets10.1016/j.msea.2009.05.017 ↗
18. Characterization of Al/Ni multilayers and their application in diffusion bonding of TiAl to TiC cermet10.1016/j.tsf.2012.01.001 ↗
19. Influence of Zn content on wettability of TiC cermet by AgCuZn alloy
20. Influence of Zn addition on wettability of AgCu brazing alloy on TiC cermet
21. Microstructures of eutectic and near eutectic specimens in the ternary Ag-Cu-Zn system10.1179/cmq.1980.19.4.345 ↗
22. Kinetics of wetting and spreading of AgCu filler metal over Ti–6Al–4V substrates10.1007/s10853-016-0308-7 ↗
23. The relation between wetting and interfacial chemistry in the CuAgTi/alumina system10.1016/j.actamat.2005.11.048 ↗
24. Reactive wetting in titanium carbide/non-reactive metal systems10.1016/j.cossms.2006.02.008 ↗
25. The spreading kinetics of Ag-28Cu (L) on nickel (S): Part I. Area of spread tests on nickel foil10.1557/JMR.1996.0241 ↗
26. Nonreactive wetting kinetics of binary alloys: a molecular dynamics study10.1016/j.actamat.2010.10.039 ↗
27. Phase equilibria of the ternary Ag-Cu-Ni system and the interfacial reactions in the Ag-Cu/Ni couples10.1007/BF00355906 ↗
28. Chang · 1979
29. Liquid-solid phase distribution studies in the systems iron-lead, cobalt-lead, chromium-tin, and nickel-silver
30. Hultgren · 1973
31. Thermodynamic description of the Cu-Ni-Zn system above 600°C10.1016/j.calphad.2003.09.002 ↗
32. The rate of solution of solid substances in their own solutions10.1021/ja02086a003 ↗
33. Forced wetting of a reactive surface10.1016/j.cis.2012.06.002 ↗
34. Contact angle and local wetting at contact line10.1021/la3036456 ↗
35. Forced wetting dynamics: a molecular dynamics study10.1021/la020724j ↗
36. Influence of solid–liquid interactions on dynamic wetting: a molecular dynamics study10.1088/0953-8984/21/46/464124 ↗