journal article·2014-01

Structural and electrical properties of SnO2 films grown on r-cut sapphire at different substrate temperature by MOCVD

Caina Luan, Zhen Zhu, Wei Mi, Jin Ma

Vacuum· Volume 99
Publisher page

Abstract

Abstract Tin oxide (SnO2) films have been grown on r-cut sapphire substrates by metalorganic chemical vapor deposition (MOCVD). The substrate temperature dependent structural and electrical properties of SnO2 films were investigated. It was found that the films deposited at lower temperatures were polycrystalline while the highly oriented growth occurred above 600 °C. Especially, high-quality SnO2 film with no (101) twin structure was obtained at 700 °C. Scanning electron microscopy showed that the surface morphology was significantly affected by the substrate temperature. A tile-like surface was observed for the film grown at 700 °C. The change in electrical properties for the SnO2 films was associated with the various structures at different substrate temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Gas Sensing Nanomaterials and Sensors · ZnO doping and properties · Transition Metal Oxide Nanomaterials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Norton · Mater Sci Eng R-Rep · 2004 · 43 · 13910.1016/j.mser.2003.12.002 ↗
2. He · J Alloys Compd · 2011 · 509 · L1110.1016/j.jallcom.2010.09.112 ↗
3. Yang · Appl Surf Sci · 2009 · 255 · 440110.1016/j.apsusc.2008.10.129 ↗
4. Yakuphanoglu · J Alloys Compd · 2009 · 470 · 5510.1016/j.jallcom.2008.03.013 ↗
5. Batzill · Prog Surf Sci · 2005 · 79 · 4710.1016/j.progsurf.2005.09.002 ↗
6. Watson · Sens Actuators · 1984 · 5 · 2910.1016/0250-6874(84)87004-3 ↗
7. Elangovan · J Cryst Growth · 2005 · 276 · 21510.1016/j.jcrysgro.2004.11.387 ↗
8. Kim · J Alloys Compd · 2006 · 426 · 28610.1016/j.jallcom.2006.01.093 ↗
9. Zhang · Adv Mater · 2003 · 15 · 102210.1002/adma.200304899 ↗
10. Liu · J Mater Res · 1995 · 10 · 151610.1557/JMR.1995.1516 ↗
11. Sundqvist · Thin Solid Films · 2006 · 514 · 6310.1016/j.tsf.2006.02.031 ↗
12. Wen · J Alloys Compd · 2010 · 508 · 37010.1016/j.jallcom.2010.08.034 ↗
13. Sundqvist · Chem Vap Deposition · 2004 · 10 · 7710.1002/cvde.200306279 ↗
14. Batzill · Thin Solid Films · 2005 · 484 · 13210.1016/j.tsf.2005.02.016 ↗
15. Dominguez · J Appl Phys · 2002 · 91 · 106010.1063/1.1426245 ↗
16. Lu · J Cryst Growth · 2004 · 260 · 19110.1016/j.jcrysgro.2003.08.042 ↗
17. Zhu · J Luminescence · 2011 · 131 · 8810.1016/j.jlumin.2010.09.004 ↗
18. McCarthy · Powder Diffr · 1989 · 4 · 15610.1017/S0885715600016638 ↗
19. Chu · 1978
20. Yadav · J Alloys Compd · 2009 · 488 · 35010.1016/j.jallcom.2009.08.130 ↗
21. Tien · Mater Res Bull · 2009 · 44 · 610.1016/j.materresbull.2008.09.010 ↗
22. Feng · Mater Lett · 2008 · 62 · 180910.1016/j.matlet.2007.10.007 ↗
23. Robertson · J Phys Rev B · 1984 · 30 · 352010.1103/PhysRevB.30.3520 ↗
24. Samson · J Appl Phys · 1973 · 44 · 461810.1063/1.1662011 ↗