journal article·2020-04

Strengthening and toughening effects in laves phase Cr2Ta/Cr in-situ composites by Si additions

Yunlong Xue, Shuangming Li, Yuanting Wu, Changqing Liu, Hulin Liu, Liang Yuan

Vacuum· Volume 174
Publisher page

Abstract

Abstract Three Cr–8Ta-xSi (x = 0, 6, 10) (at.%) alloys were fabricated by vacuum non-consumable arc melting in this study to investigate the microstructure evolutions and mechanical properties of the Si-modified Cr2Ta/Cr in-situ composites. The element Si was incorporated preferentially into Cr2Ta rather than phase Cr, thus the microstructure transited from the dendrite Cr plus the eutectic Cr2Ta/Cr in the Cr–8Ta alloy, to the full eutectic Cr2Ta/Cr in the Cr–8Ta–6Si alloy, and finally to the dendrite Cr2Ta plus the eutectic Cr2Ta/Cr in the Cr–8Ta–10Si alloy. The Cr–8Ta–6Si alloy was developed with a good combination of strength and toughness, and the yield strength and fracture toughness of this alloy reached up to 960 ± 20 MPa and 15 ± 0.3 MPa m1/2, respectively. The good combination of strength and toughness in the Cr–8Ta–6Si alloy resulted from the synergistic effects of solid solution strengthening, alloying toughening, interface strengthening and second phase toughening.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Titanium Alloys Microstructure and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Basal slip in Laves phases: the synchroshear dislocation10.1016/j.scriptamat.2019.03.016 ↗
2. First-principles studies of the structural and electronic properties of the C14 Laves phase XCr2 (X=Ti, Zr, Nb, Hf and Ta)10.1080/14786435.2013.778427 ↗
3. A two-dimensional structure map for prediction of the transition-metal Laves phases10.1016/j.commatsci.2016.08.023 ↗
4. Effect of Mo on the microstructure and oxidation behavior of hot-pressed TaCr2 alloys10.1007/s11041-019-00409-y ↗
5. First-principles studies on structural and electronic properties of TaCr2 Laves phase10.1016/j.physb.2010.07.025 ↗
6. Microstructure and mechanical properties of two-phase Cr-Cr2Ta alloys10.1007/s11661-012-1140-6 ↗
7. Effects of Ru additions on microstructure and mechanical properties of Cr-TaCr2 alloys10.1016/j.intermet.2004.07.017 ↗
8. Oxidation resistance and mechanical properties of Laves phase reinforced Cr in-situ composites10.1016/S0966-9795(00)00046-7 ↗
9. Plastic-deformation mechanism in complex solids10.1038/nmat2713 ↗
10. Effects of Fe additions on the mechanical properties and oxidation behavior of Cr2Ta Laves phase reinforced Cr10.1016/j.scriptamat.2005.01.016 ↗
11. Microstructure and mechanical properties of Cr-Ta-Si Laves phase-based alloys at elevated temperatures10.1080/14786435.2014.971086 ↗
12. Effects of Si additions on the high temperature oxidation behavior of Cr-Cr2Ta alloys10.1016/j.intermet.2012.09.013 ↗
13. Characterization of fracture toughness and toughening mechanisms in Laves phase Cr2Nb based alloys10.1016/j.msea.2015.04.077 ↗
14. Brown · 1993
15. First-principles density functional theory study of phase transformations in NbCr2 and TaCr210.1016/j.actamat.2008.06.014 ↗
16. The kinetics of a polytypic Laves phase transformation in TiCr210.1016/j.intermet.2010.11.027 ↗
17. Polytypic transformations in Laves phases10.1016/j.intermet.2004.02.017 ↗
18. A study on the influence of Mo, Al and Si additions on the microstructure of annealed dual phase Cr-Ta alloys10.1007/s10853-012-7114-7 ↗
19. Bhowmik · Intermetallics · 2014 · 48 · 6210.1016/j.intermet.2013.11.002 ↗
20. On the fracture and fatigue properties of Mo-Mo3Si-Mo5SiB2 refractory intermetallic alloys at ambient to elevated temperatures (25°C to 1300°C)10.1007/s11661-003-0325-4 ↗
21. Nanoindentation study on solid solution softening of Fe-rich Fe2Nb Laves phase by Ni in Fe-Nb-Ni ternary alloys10.1016/j.intermet.2015.11.003 ↗
22. Plastic deformation of single crystalline C14 Mg2Ca Laves phase at room temperature10.1016/j.msea.2019.05.092 ↗
23. Spark plasma sintering and microstructural characterization of Nb-Cr eutectic alloy
24. Laves phase intermetallic matrix composite in situ toughened by ductile precipitates10.1016/j.scriptamat.2017.06.043 ↗
25. Microstructures and defect structures in ZrCr2 Laves phase based intermetallic compounds10.1016/S0966-9795(02)00057-2 ↗
26. The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron10.1007/BF02642799 ↗
27. Microstructures and compressive properties of NiAl-Cr(Mo) and NiAl-Cr eutectic alloys with different Fe contents10.1016/j.msea.2018.12.085 ↗
28. A true change of NiAl-Cr(Mo) eutectic lamellar structure during high temperature treatment10.1016/j.jallcom.2017.10.159 ↗