An investigation of thermal-mechanical interaction effect on PVD coated tool wear for milling Be/Cu alloy
Source abstract
Abstract
Abstract In this paper, a comparative study is reported on tool wear morphology described by machining Be/Cu alloy at different cutting speed:200 m/min,400 m/min,600 m/min,800 m/min and 1000 m/min. The cemented tungsten carbide tools, both coated with TiAlN, are used to test tool life, and the flank wear extent and standard deviation are adopted to describe surface wear pattern. In order to explain the wear mechanism under different cutting speed, a series of theoretical calculation and experiment results were listed in this paper to explain adhesive effect on tool wear under different surface pressure, and results show that the adhesions and wear patterns would be affected by cutting speed and surface pressure. Comparing the relationship between cutting force, cutting heat, surface elements and tool wear, we can easily find out that the hard particle such as Cu and Be adhered to cutting edge to affect tool geometry and strengthen. Besides, the microstructure and generation probability are analyzed to discuss the crystal surface slipping effect on tool wear.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced machining processes and optimization · Advanced materials and composites · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Microstructure and mechanical properties of copper-titanium-nitrogen multiphase layers produced by a duplex treatment on C17200 copper-beryllium alloy10.1016/j.matdes.2015.06.130 ↗
2. An investigation of tool and hard particle interaction in nanoscale cutting of copper beryllium10.1016/j.commatsci.2018.01.011 ↗
3. Wear mechanisms of uncoated and coated cemented carbide tools in machining lead-free silicon brass10.1016/j.wear.2017.01.039 ↗
4. High temperature plasma nitriding to modify Ti coated C17200 Cu surface: microstructure and tribological properties10.1016/j.vacuum.2017.10.011 ↗
5. Corrosion behavior of TaC/Ta composite coatings on C17200 alloy by plasma surface alloying and CVD carburizing10.1016/j.surfcoat.2018.12.074 ↗
6. An investigation of cutting force and tool wear in turning of Haynes 282[J]10.1016/j.jmapro.2018.12.025 ↗
7. Influence of tool wear on machining forces and tool deflections during micro milling
8. Wear resistance of TiN(Ti2N)/Ti composite layer formed on C17200 alloy by plasma surface Ti-alloy and nitriding10.1016/j.apsusc.2016.03.059 ↗
9. Microstructural characteristics of alloy 718 and Waspaloy and their influence on flank wear during turning10.1016/j.wear.2018.01.011 ↗
10. Wear performance and mechanisms of PCBN tool in dry hard turning of AISI D2 hardened steel10.1016/j.triboint.2018.12.026 ↗
11. Investigation of tool wear in the turning of Inconel 718 superalloy in terms of process performance and productivity enhancement10.1016/j.triboint.2017.10.005 ↗
12. Study on the tool wear and its effect of PCD tool tool in micro milling of tungsten carbide10.1016/j.ijrmhm.2018.07.010 ↗
13. The effect of sliding speed on the wear steel-tool steel pairs10.1016/j.triboint.2016.01.030 ↗
14. Crater and flank wear resistance of cutting tools having micro textured surfaces10.1016/j.precisioneng.2013.05.007 ↗
15. Tool wear behaviors and corresponding machined surface topography during high-speed machining of Ti-6Al-4V with fine gain tools10.1016/j.triboint.2018.01.057 ↗
16. Adhesion and wear properties of boro-tempered ductile iron10.1016/j.matdes.2011.04.014 ↗
17. Thermal modeling of the metal cutting process Part I- Temperature rise distribution due to shear plant heat source10.1016/S0020-7403(99)00070-3 ↗
18. Thermal analysis of high efficiency deep grinding10.1016/S0890-6955(00)00074-2 ↗
19. Thermal modeling for white layer predictions in finish hard turning10.1016/j.ijmachtools.2004.09.006 ↗
20. Tool wear behavior of thermal-mechanical effect for milling Ti-6Al-4V alloy in cryogenic[J]10.1007/s00170-017-1012-8 ↗
21. Zhang · 1990 · 101
22. Ding · 1989 · 198
23. Thomas · 2000 · 34