Preparation and thermoelectric properties of nc-Si:(Al2O3+SiO2) composite film
Source abstract
Abstract
Abstract A composite film of nanocrystalline Si (nc-Si) embedded in (Al 2 O 3 + SiO 2 ) has been prepared on a quartz substrate by thermally evaporating a 400 nm thick Al film on a quartz substrate and annealing in air at 580 °C for 1 h. During annealing, the Al reacts with the SiO 2 of the quartz substrate and produces nc-Si, which is embedded in the (Al 2 O 3 + SiO 2 ) film. The average size of nc-Si is ~ 22 nm and the thickness of the nc-Si:(Al 2 O 3 + SiO 2 ) composite film is ~ 810 nm. It is found that the prepared film is thermoelectric with a Seebeck coefficient of − 624 μV/K at 293 K and − 225 μV/K at 413 K.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Semiconductor materials and interfaces · Thermal properties of materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References