Phosphorus doping of silicon at substrate temperatures above 600°C

Philip E. Thompson, Glenn G. Jernigan, David S. Simons, P. Chi, Berend T. Jonker, O.M.J. van ‘t Erve

Publisher page

Abstract

Abstract Phosphorus doping of silicon during growth by molecular beam epitaxy (MBE) has been investigated in the temperature regime 700 °C to 870 °C. By designing a growth sequence that fully accounts for the P deposited in a delta-doped layer, and then tracks the P as it segregates into the undoped Si and traps the surface P in a low temperature Si cap, it was determined that the onset of significant P evaporation during growth occurred at a substrate temperature of 663 °C ± 10 °C. The P sublimation process had an activation energy of 199 kJ/mol ± 22 kJ/mol.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · Advancements in Semiconductor Devices and Circuit Design · Silicon and Solar Cell Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.