Grain size, texture, and crystallinity in lanthanum monosulfide thin films grown by pulsed laser deposition
Source abstract
Abstract
Abstract We report a detailed investigation of the growth of lanthanum monosulfide (LaS) thin films by pulsed laser deposition on (001) magnesium oxide (MgO) substrates in a background of H 2 S for the purpose of optimizing their crystallinity, texture, and grain size. A variety of films were grown while varying the laser repetition rate, the temperature of the substrate, and the partial pressure of H 2 S. The thin films were characterized by X-ray diffraction (XRD), atomic force microscopy (AFM), Raman spectroscopy, and high resolution transmission electron microscopy. Films grown at 500 °C with a H 2 S background pressure of 3.4 × 10 − 4 Pa and a laser repetition rate of 8 Hz produced the LaS film with the largest grains whose size averaged 293 nm. The XRD pattern of these films revealed that their orientation was predominantly (200). AFM images of the surface of these films showed large plate-like grains. This contrasts with the fine grain structure observed in LaS films grown at a lower substrate temperature and lower H 2 S pressure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic and Structural Properties of Oxides · ZnO doping and properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.