Microstructures of YBa2Cu3O7/La0.7Ca0.3MnO3 and La0.7Ca0.3MnO3/YBa2Cu3O7 bi-layers grown on (001)LaAlO3
Source abstract
Abstract
Abstract Epitaxial YBa 2 Cu 3 O 7 /La 0.7 Ca 0.3 MnO 3 (YBCO/LCMO) bi-layers and La 0.7 Ca 0.3 MnO 3 /YBa 2 Cu 3 O 7 (LCMO/YBCO) bi-layers were grown on (001)LaAlO 3 by pulsed laser deposition, and their microstructures were compared by transmission electron microscopy investigation. In the YBCO(100 nm)/LCMO(150 nm) bi-layers, the LCMO layer consists of columnar grains of ~ 17 nm in diameter and contains mixed orientation domains of [100] c , [010] c and [001] c . The YBCO layer is totally c -axis oriented and the YBCO lattices are tilted − 2.5° to + 2.5° as they grew on the rough surfaces of LCMO columnar grains. For the LCMO(140 nm)/YBCO(140 nm) bi-layers, the LCMO/YBCO interface is sharp and flat. The initial 12-nm thickness of the YBCO layer is composed of c -axis oriented domains, and the upper part of YBCO layer is [100] oriented. The LCMO layer was predominantly [001] c oriented while [100] c -oriented domains were occasionally observed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic and transport properties of perovskites and related materials · Physics of Superconductivity and Magnetism · Advanced Condensed Matter Physics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.