Reduction of surface recombination velocity by rapid thermal annealing of p-Si passivated by catalytic-chemical vapor deposited alumina films

Yoh-Ichiro Ogita, Masayuki Tachihara

Publisher page

Abstract

Abstract Excellent electrical-passivation of p-type Si (p-Si) in Si solar cells has been achieved by post-deposition rapid annealing of aluminum oxide (AlOx) films prepared by catalytic chemical vapor deposition (Cat-CVD) using trimethyl aluminum (TMA) and O2. Extremely small surface recombination velocity of below 0.1 cm/s has been obtained at post-deposition annealing temperatures in the range of 350–400 °C for an annealing time of 2 min. The reduction of surface recombination velocity has been attributed to band bending induced by a fixed negative charge density of 5 × 1011 charges/cm2 and an additional small interface trapping density of around 1010 cm− 2 eV− 1.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.