Abstract La 0.7 Sr 0.3 MnO 3 thin films were deposited on SiO 2 /Si substrates by RF magnetron sputtering under different oxygen gas flow rates with a sputtering power of 100 W. During deposition, the substrate was heated at 623 K. To investigate post-annealing effects, the as-deposited La 0.7 Sr 0.3 MnO 3 thin films were thermal-treated at 973 K for 1 h. The effects of oxygen gas flow rate and post-annealing treatment on the physical properties of the films were systematically studied. X-ray diffraction results show that the growth orientation and crystallinity of the films were greatly affected by the oxygen gas flow rate and substrate heating during deposition. The sheet resistance of the films gradually decreased with increasing oxygen gas flow rate, while the post-annealed films showed the opposite behavior. The temperature coefficient of resistance at 300 K of La 0.7 Sr 0.3 MnO 3 thin films deposited at an oxygen gas flow rate of 40 sccm decreased from − 2.40%/K to − 1.73%/K after post annealing. The crystalline state of the La 0.7 Sr 0.3 MnO 3 thin films also affected its electrical properties.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic and transport properties of perovskites and related materials · Rare-earth and actinide compounds · Magnetic Properties of Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.