Deposition of Li4Ti5O12 and LiMn2O4 films on the lithium-ion conductor of Li1.3Al0.3Ti1.7(PO4)3 sintered pellet

Xian Wu, Shang Chen, Ze He, Shou Bin Chen, Run Xiu Li

Publisher page

Abstract

Abstract LiMn2O4 and Li4Ti5O12 films were deposited on the lithium-ion conductor of Li1.3Al0.3Ti1.7(PO4)3 sintered pellet by spray technique. The effect of annealing temperature, annealing time, Li:Ti and Li:Mn molar ratio on the phase and crystallization of the films were investigated with X-ray diffraction. The LiMn2O4/Li1.3Al0.3Ti1.7(PO4)3/Li4Ti5O12 thin-film lithium-ion battery using Li1.3Al0.3Ti1.7(PO4)3 sintered pellet as both electrolyte and substrate was also studied. The results show that the effect of annealing temperature, annealing time, Li:Ti and Li:Mn molar ratio has great effect on the phase and crystallization of Li4Ti5O12 and LiMn2O4 films deposited on the Li1.3Al0.3Ti1.7(PO4)3 sintered pellet. The optimal Li:Ti and Li:Mn molar ratio for the deposition of Li4Ti5O12 and LiMn2O4 films on Li1.3Al0.3Ti1.7(PO4)3 sintered pellet are 7.2:5 and 1.05:2, respectively. The optimal annealing temperature and time for the deposition of LiMn2O4 film on Li1.3Al0.3Ti1.7(PO4)3 sintered pellet are 650 °C and 10 min. While those for Li4Ti5O12 film are 700 °C and 10 min. The LiMn2O4/Li1.3Al0.3Ti1.7(PO4)3/Li4Ti5O12 thin-film battery offers a working voltage about 2.25 V and can be easily cycled.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.