Low-temperature sol–gel intermediate layer wafer bonding

S. S. Deng, Cher Ming Tan, Jun Wei, Wei Yu, Mui Ling Sharon Nai, Hua Xie

Publisher page

Abstract

Abstract Silicon-to-silicon wafer bonding has been successfully performed using sol–gel intermediate layer, which is deposited by spinning acid-catalyzed tetraethylthosilicate solution on the surfaces of two silicon wafers to be bonded. The bond strength is up to 35 MPa at a bonding temperature of 100 °C, which is near to the fractured strength of bulk silicon. To investigate the effects of the press parameters, Draper–Lin small composite design is used, as it requires the minimum number of runs in the design of experiments. Statistic analysis shows that the bonding temperature is the dominant factor for the bond quality, while the interaction between bonding temperature and concentration is significant on bond strength. The physical mechanisms of the observed significant effects are discussed. The improvement of the wafer bonding using annealed sol–gel intermediate layer is also proposed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: 3D IC and TSV technologies · Electronic Packaging and Soldering Technologies · Synthesis and properties of polymers

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.