Pulsed laser crystallization of very thin silicon films
Source abstract
Abstract
Abstract We report 308-nm-pulsed-XeCl-excimer laser annealing of 2.2-nm-thick silicon films formed on quartz substrates. Crystallization occurred at laser energy of 150∼170 mJ/cm 2 . Raman scattering spectra revealed mixed states of small crystalline grains and disordered amorphous regions. Broad optical extinction coefficient was obtained for wavelength from 250 to 400 nm, although it was similar to that of crystalline silicon for wavelength longer than 400 nm. Blue-green photoluminescence was observed for the films annealed at 260 °C for 3 h in 1.3×10 6 Pa H 2 O vapor after crystallization.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon Nanostructures and Photoluminescence · Thin-Film Transistor Technologies · Laser Material Processing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.