article·2011-01-20

Crystallization temperature and activation energy of as-spun Ti52.0Ni38.5Cu9.5 ribbon

Kao‐Hao Chang, S.K. Wu, Shih-Hang Chang

Publisher page

Abstract

This study investigated the crystallization temperature and activation energy of as-spun Ti 52.0 Ni 38.5 Cu 9.5 ribbon. The as-spun Ti 52.0 Ni 38.5 Cu 9.5 ribbon is partially crystallized and its wave number Q p is lower than those of normal Ti-Ni binary amorphous alloys. The crystallization activation energy E a of the as-spun Ti 52.0 Ni 38.5 Cu 9.5 ribbon obtained by Kissinger's method is 422 kJ/mol. Both the thermal stability and the onset crystallization temperature of the as-spun Ti 52.0 Ni 38.5 Cu 9.5 ribbon are all lower than those of reported Ti-Ni/Ti-Ni-Cu amorphous films/ribbons. The as-spun Ti 52.0 Ni 38.5 Cu 9.5 ribbon is fully crystallized after annealing at 700 °C for 1 h and exhibits a B2⇔B19⇔B19' transformation. The ribbon annealed at 700 °C for 24 h shows two B2⇔B19 transformations because it has the mixed microstructure of large and small grains.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Shape Memory Alloy Transformations · Electromagnetic wave absorption materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.