Excimer UV-assisted preparation of zirconium silicate layers
Source abstract
Abstract
UV exposure of zirconium sol-gel layers on Si with 5, 15, 25 at.% Zr at 400°C in O 2 for 20 min has led to the formation of high quality Zr silicate layers exhibiting low-leakage current densities of 3x10 -5 A/cm 2 at 1 MV/cm for the 5% Zr layers, and even lower values of 9x10 -7 and 2x10 -7 A/cm 2 for the 15 and 25% Zr silicate layers, respectively. Annealing of these UV irradiated samples for 30 s at 1050°C in a N 2 gas flow did not cause significant changes in leakage current density at biases up to 0.7 MV/cm. The formation of Si-O-Zr bonds led to a shift of the Si-O stretching vibration towards lower wavenumbers from 1050 to 1016/cm. X-ray diffraction analyses showed that these Zr silicate layers assumed an amorphous structure after UV exposure at 400°C, and remained amorphous and stable following the high-temperature annealing at 1050°C without separating into phases of crystalline ZrO 2 and SiO 2 .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and devices · Advanced ceramic materials synthesis · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.