Near-interfacial delamination failures observed in ion-beam-sputtered Ta2O5/SiO2 multi-layer stacks
Source abstract
Abstract
Abstract Ion-beam-sputtered Ta 2 O 5 /SiO 2 multi-layer stacks have been mechanically stressed to failure. The delamination failures do not occur precisely at the layer interfaces. XPS and AFM analyses indicate that the failures occur near the interfaces where SiO 2 was deposited on Ta 2 O 5 . Delamination is not observed near the interfaces where Ta 2 O 5 was deposited on SiO 2 . The failure location is 2–3 nm into Ta 2 O 5 layers and can occur randomly near multiple interfaces within a test. The delamination failures were induced by performing tape pull tests over lines scribed into the multi-layer coatings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Semiconductor materials and devices · Copper Interconnects and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.