Crystallized SrFeO3−x films deposited by pulsed laser ablation without in-situ substrate heating
Source abstract
Abstract
Abstract Crystallized SrFeO 3− x (0≤ x ≤0.5) films were deposited by pulsed laser ablation without in-situ substrate heating with the third harmonic of a Nd:YAG laser and off-axis configuration. The crystallinity of SrFeO 3− x films strongly depended on the ambient pressure of Ar gas. The films deposited are amorphous below 10 Pa, and crystalline from 10 to 200 Pa. The films deposited at 30 Pa have the optimum stoichiometry of Sr to Fe, approximately 1.05. A stoichiometric and well-crystallized SrFeO 3 film with a smooth surface was fabricated by post-annealing (300 °C in air) the amorphous films deposited at 1 Pa.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic and transport properties of perovskites and related materials · Electronic and Structural Properties of Oxides · Multiferroics and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.