Abstract

Abstract Single-, 15-, and 30-layered Cr–N coatings deposited on a steel substrate were oxidized in air at 700 and 800 °C. Oxidation occurred via the predominant outward diffusion of Cr, Fe, and nitrogen, and the inward diffusion of oxygen. Nitrogen escaping from the coating into the air made the multi-layered Cr–N coating act as a single-layered Cr–N coating during oxidation. The oxidation product was primarily Cr 2 O 3 , which contained a small amount of Fe and nitrogen. The unreacted coating beneath the Cr 2 O 3 scale had some iron transported from the substrate.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. Navinsek · Surf. Coat. Technol. · 1993 · 59 · 24410.1016/0257-8972(93)90091-2 ↗
2. Kacsich · J. Phys., Condens. Matter · 1996 · 8 · 1070310.1088/0953-8984/8/49/055 ↗
3. Huber · Surf. Coat. Technol. · 1994 · 68/69 · 6410.1016/0257-8972(94)90139-2 ↗
4. Wang · J. Electrochem. Soc. · 2003 · 150 · B19910.1149/1.1563649 ↗
5. Mayrhofer · Surf. Coat. Technol. · 2001 · 146/147 · 22210.1016/S0257-8972(01)01471-2 ↗
6. Ichimura · J. Mater. Res. · 1994 · 9 · 15110.1557/JMR.1994.0151 ↗
7. Lee · Surf. Coat. Technol. · 2001 · 141 · 22710.1016/S0257-8972(01)01238-5 ↗
8. Hsieh · J. Electrochem. Soc. · 2002 · 149 · B23410.1149/1.1471545 ↗
9. Myung · Mater. Lett. · 2004 · 58 · 151310.1016/j.matlet.2003.10.021 ↗
10. Kofstad · Oxid. Met. · 1995 · 44 · 310.1007/BF01046721 ↗