article·2000-09-01

The influence of TiB2-thin film thickness on metal–GaAs structural characteristics

T. Kryshtab, Jesús Palacios Gómez, P. M. Lytvyn, O. S. Lytvyn

Publisher page

Abstract

Abstract X-Ray diffraction and atomic force microscopy structural properties investigations of TiB 2 /GaAs device structures as-produced and annealed have been carried out. The samples were obtained by magnetron sputtering on Czochralski-grown (001) GaAs substrates doped by Te up to a concentration of 10 18 cm −3 . The magnetron sputtering was carried out in an argon atmosphere at pressure in the chamber of 5×10 −3 torr. The currents of sputtering were 0.3 A and 0.4 A and the thickness of TiB 2 -films was from 10 nm to 50 nm. The short-term annealing of the samples was carried out in a stream of hydrogen in the furnace at temperatures 400, 600 and 800°C during 1 min with a heating velocity of 1800°C/min. The TiB 2 -film thickness and magnetron sputtering current determined the grain size and surface roughness as well as interface structural parameters. At sputtering current 0.4 A, some process of film texturing takes place. The residual strains in the film increase with a rise in the sputtering current. The structural relaxation at annealing is exhibited in decreasing of residual strains as well as film recrystallization and transformation of surface morphology. The dependence of these processes on annealing temperature does not have monotonous character and differs for various thicknesses of TiB 2 -film.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References