Effect of Ti alloying in nickel silicide formation
Source abstract
Abstract
Abstract In the presence of interfacial oxide, an addition of 20 at.% Ti to Ni film leads to the formation of a thick TiOx layer at the Ni(Ti)/Si interface upon annealing, preventing the inter-diffusion of Ni and Si hence hindering the Ni silicide formation up to 700 °C. At 800 °C, a mixture of predominant NiSi phase with some NiSi2 grains facetted in (111) plane was observed. A different mechanism occurred for the sample with minimal oxygen contamination where Ni3Si2 was found to be stable up to 900 °C. Nevertheless, Ti addition has delayed the silicidation reaction to 600 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and interfaces · Silicon and Solar Cell Technologies · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.