Phase transformation and hardness of the Ni–P–Al ternary coatings under thermal annealing
Source abstract
Abstract
Ternary Ni-P-Al coatings were fabricated by the dual-gun rf magnetron sputtering technique. The as-deposited Ni-P-Al coatings exhibited a major Ni nanocrystalline phase (with a (111) texture) with Al and P co-deposited. After 400 °C heat treatment, various Ni x P y compounds, including Ni 12 P 5 , Ni 5 P 2 , and Ni 3 P, formed within the recrystallized Ni matrix. Accordingly, the hardness of the coating increased to 10 GPa due to the Ni x P y precipitation. For heat treatment temperatures higher than 450 °C, Ni p Al q hard phases were observed in the ternary Ni-P-Al coating. A further increase in coating hardness from 10 to 12 GPa was revealed. The hardening of the annealed Ni-P-Al coatings was attributed to precipitation of Ni-P and Ni-Al compounds formed around 400 and 500 °C, respectively. A two-stage hardening in Ni-P-Al coating by Ni x P y and Ni p Al q precipitation through heat treatment was then demonstrated. Through surface analysis, the increase in surface roughness for the Ni-P-Al coating due to the formation of Ni x P y and Ni p Al q compounds was revealed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Metallurgical and Alloy Processes · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Sue · Surf. Coat. Technol. · 1995 · 76–77 · 6110.1016/0257-8972(95)02506-5 ↗
2. Spencer · Met. Finish. · 1974 · 35
3. Chiba · J. Mater. Res. · 1993 · 8 · 110910.1557/JMR.1993.1109 ↗
4. Ramalingam · Wear · 1984 · 118 · 335
5. Dennis · 1986 · 276
6. Wang · 1992 · 57
7. Nash · 1991 · 235
8. Armyanov · J. Electrochem. Soc. · 1996 · 143 · 369210.1149/1.1837273 ↗
9. Boanani · J. Appl. Electrochem. · 1999 · 29 · 63710.1023/A:1026441403282 ↗
10. Schlesinger · J. Electrochem. Soc. · 1990 · 137 · 1858.J10.1149/1.2086818 ↗
11. Zhang · Mater. Charact. · 1996 · 37 · 11910.1016/S1044-5803(96)00089-7 ↗
12. Aoki · Plating Surf. Finish. · 1990 · 48
13. Zhang · Trans. IMF · 1996 · 74 · 6910.1080/00202967.1996.11871098 ↗
14. Tsai · Surf. Coat. Technol. · 2001 · 146–147 · 50210.1016/S0257-8972(01)01462-1 ↗
15. Chang · Surf. Coat. Technol. · 2001 · 139 · 23310.1016/S0257-8972(01)01009-X ↗
16. Wu · Surf. Coat. Technol. · 2002 · 150 · 23210.1016/S0257-8972(01)01514-6 ↗
17. Chen · Surf. Coat. Technol. · 2004 · 177–178 · 22210.1016/j.surfcoat.2003.09.036 ↗
18. Wu · Thin Solid Films · 2003 · 441 · 16510.1016/S0040-6090(03)00970-2 ↗
19. Wu · Surf. Coat. Technol. · 2004 · 177–178 · 31210.1016/j.surfcoat.2003.09.010 ↗
20. Lin · Surf. Coat. Technol. · 2004 · 188–189 · 49510.1016/j.surfcoat.2004.08.062 ↗
21. Goldstein · 1981
22. Wu · Surf. Coat. Technol. · 2003 · 166 · 6010.1016/S0257-8972(02)00725-9 ↗