Preparation of sub-nanometer thickness-controlled tin dioxide films by pulsed atomic-layer CVD
Source abstract
Abstract
Abstract Tin dioxide coatings of sub-nanometer thickness on glass were prepared between 325 and 525 °C by pulsed atomic-layer chemical vapor deposition. The sample films grown on substrates at 400 to 450 °C exhibited a constant growth rate of 1.6 A/cycle, corresponding to one-fourth the length of tin dioxide (110) lattice spacings. We propose herein a dry method of thickness measurement for very thin, sub-nanometer-thick films based on X-ray photoelectron spectroscopy depth profiles using argon ion sputtering and etching time values calibrated using both stylus and optical interference methods for tin dioxide films. The preferred orientations of the films are (110) and (100), and the tentative grain size is 80×100 nm for 10-nm-thick films. Optical transmittance for visible light exceeds 0.9, and optical absorption edges at room temperature occur at 3.75 eV. Ultra-violet photoelectron spectroscopy (UPS) measurements of the electronic density of states are performed on as-grown films surfaces.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · Transition Metal Oxide Nanomaterials · Ga2O3 and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.