High rate deposition and electron beam recrystallization of silicon films for solar cells
Source abstract
Abstract
Abstract Silicon films were deposited onto graphite substrates by means of a plasma-enhanced chemical vapor deposition (PECVD) process from trichlorosilane (SiHCl 3 ) hydrogen gas mixtures at a substrate temperature of 450°C. The plasma was operated at a frequency of 13.56 MHz and a pressure of 500 Pa. Deposition rates of 340 nm min −1 and greater were achieved. The films were examined by optical and scanning electron microscopy, X-ray diffractometry and elastic-recoil detection analysis. The as-deposited films were nanocrystalline. They were then recrystallized by means of a zone melting process realized by a line-shaped electron beam being scanned over the surface. To achieve sufficient wettability during recrystallization, methane (CH 4 ) was added to the atmosphere at the beginning of plasma-enhanced deposition. The films obtained had a polycrystalline structure with a typical grain size of 100 μm in width (i.e. perpendicular to the direction of scanning) and up to several mm in length. The chlorine content of the silicon films was significantly reduced by recrystallization; impurities of hydrogen and oxygen also decreased, while the carbon content increased.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Thin-Film Transistor Technologies · Silicon and Solar Cell Technologies · Silicon Nanostructures and Photoluminescence
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.