Application of SiO2 aerogel film for interlayer dielectric on GaAs with a barrier of Si3N4
Source abstract
Abstract
Si3N4 film was adopted as a barrier layer for SiO2 aerogel/GaAs system. Si3N4/GaAs formed an almost chemically sharp interface and nearly maintained their chemical inertness during in-situ heating until 400 °C under ultra high vacuum condition. One micrometer thick SiO2 aerogel film was prepared on the Si3N4/GaAs system using supercritical drying procedure at 250 °C and under 1160 psi. The thickness of Si3N4 barrier layer was varied as 400, 600 and 900 A. The dielectric constant of all SiO2 aerogel/Si3N4/GaAs system was measured as approximately 1.9 and almost no difference was observed from the changes in the thickness of Si3N4 barrier layer. The leakage current densities were measured as low as under 2×10−7 A/cm2 and these values are two orders smaller than that of SiO2 aerogel/GaAs system prepared without the introduction of Si3N4 barrier layer. All the aerogel/Si3N4/GaAs systems show ohmic conduction at low applying field and space charge limited conduction at high applying field. Furthermore, a reduced leakage current behavior was observed with increased Si3N4 layer thickness and could be explained from the electric-field depression effect due to accumulated charges in the films.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Synthesis and properties of polymers · Semiconductor materials and devices · Aerogels and thermal insulation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References