article·2006-04-18

The large modification of phase transition characteristics of VO2 films on SiO2/Si substrates

Ningyi Yuan, Jinhua Li, Ge Li, Xiaoshuang Chen

Publisher page

Abstract

Abstract The vanadium oxide (VO 2 ) films have been prepared on SiO 2 /Si substrates by using a modified Ion Beam Enhanced Deposition (IBED) method. During the film deposition, high doses of Ar + and H + ions have been implanted into the deposited films from the implanted beam. The resistance change of the VO 2 films with temperature has been measured and the phase transition process has been observed by using the X-ray Diffraction technique. The phase transition of the IBED VO 2 films starts at a low temperature of 48 °C and ends at a high temperature of 78 °C. It is found that the phase transition characteristics can be adjusted by changing the annealing temperature or the time and the phase transition characteristics of the IBED VO 2 films depend on the quantity and location of argon atoms in the film matrix.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Transition Metal Oxide Nanomaterials · Ga2O3 and related materials · ZnO doping and properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.